TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Jack Olson <[log in to unmask]>
Date:
Sat, 1 Oct 2011 17:02:04 -0700
Reply-To:
Message-ID:
<717AA2DB37EB4C2D8E625A6950EDA032@UsHiemII>
Content-Transfer-Encoding:
7bit
Subject:
From:
Ahne Oosterhof <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (125 lines)
You are correct! And the problem remains. What is a "product" to one is a
"component" to another. 

So when you buy a display card for your computer and it has a UL mark on it,
how do you know it is for the board material only?

When I buy a power cord and it has a UL label on one end, can I assume that
the connector is included? (which, by the way, is a terribly unsafe device
and acceptable to UL!).

 

As I see it, the problem is the same and at the moment unresolved.

 

Ahne.

 

  _____  

From: Jack Olson [mailto:[log in to unmask]] 
Sent: Saturday, October 01, 2011 13:54
To: [log in to unmask]
Cc: TechNet E-Mail Forum
Subject: Re: [TN] standard industry silkscreened symbology for Pb-free
assembly

 

I think it is... 

 

The UL mark only certifies that the materials used in the bare board, and
doesn't tell you anything about the assembly (I think... am I crazy?)

 

The RoHS (or now incorporated into CE) mark represents the entire product

 

Jack

On Mon, Sep 26, 2011 at 11:35 AM, Ahne Oosterhof <[log in to unmask]> wrote:

Is this problem any different than having the board manufacturer mark the
board as passing UL requirements?

Ahne.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Sunday, September 18, 2011 08:20
To: [log in to unmask]
Subject: Re: [TN] standard industry silkscreened symbology for Pb-free
assembly

I agree, but I would also caution you to think about something.
When you mark something on a bare board as being "lead free",
are you telling the world that only the bare board is lead free?
...or are you implying that the final assembly is lead free?
Be cautious about marking a bare board, and then losing control of it later
on.

Maybe the assembler should be marking the final assembly as "compliant"?

Does anyone else have experience with this?
I'm nervous about stamping a bare board, and then someone later down the
line decides to assemble the board with different criteria...

Jack

.

On Fri, 16 Sep 2011 08:52:53 -0500, Kim Sterling <[log in to unmask]>
wrote:

>Hello Joe - Our tech staff recommends IPC/J-STD-609A, IPC/JEDEC Marking and
Labeling of Components, PCBs and PCBAs to Identify Lead (Pb), Lead-Free
(Pb-Free) and Other Attributes. Written to cover this type of question.
www.ipc.org/609A<http://www.ipc.org/609A>.
>
>Hope that helps.
>
>Kim Sterling, IPC

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 <tel:847-615-7100%20ext.2815>  ext.2815
-----------------------------------------------------



 



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2