TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 27 Oct 2011 15:12:47 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, E-Mail Forum Wayne Knapp <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="UTF-8"
Content-Transfer-Encoding:
quoted-printable
From:
E-Mail Forum Wayne Knapp <[log in to unmask]>
Parts/Attachments:
text/plain (15 lines)
Hi Technetters,
I could use your help resolving an issue I’m having with the ESD bags that we are currently using for packaging. The ESD bags are sticking to the conformal coating (Solithane S-113) on the CCAs that are placed in the bag. We cannot change the coating that is used on the CCAs, so we are looking for ESD safe packaging bags that will not stick to the CCAs. Does anyone know if there is an ESD bag (material) that would not stick to the CCAs?  Any help identifying a suitable ESD bag material and supplier would be appreciated.
Thanks,
Wayne

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2