TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Reuven Rokah <[log in to unmask]>
Date:
Sun, 23 Oct 2011 09:48:13 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Message-ID:
Subject:
From:
Bev Christian <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (147 lines)
Reuven,
I respectfully disagree.  Even if we assume a peak reflow temperature for
eutectic tin/lead solder of only 205C and a high 260C for SAC305 the vapor
pressure due to trapped air and/or moisture is still not going to double.

P1V1=n1RT1
P2V2=n2RT2

R = a constant
n1 = n2
V1 = V2

Leaving 
P1/P2 = T1/T2

300/P2 = (205+273)/260+273)

P2 = 300*533/478

P2 = 334  That is only an 11% increase.

Not sure where the 300 came from in the first place, but no matter what
number you start with, it does not double.

Bev
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Reuven Rokah
Sent: Sunday, October 23, 2011 5:03 AM
To: [log in to unmask]
Subject: Re: [TN] How do we determine the Maximum Acceptable Moisture
Content (MAMC) for a board?

Hi Garcia,
You didn't mention the most important variable: the process technology, the
vapor pressure (300 to 650 psi) of Lead free is more than double than Leaded
process at the reflow peak temp.
the MAMC for Leaded process should be 0.20% and for Lead Free 0.17%. (ref.
Werner Engelmaier PCB FAB Notes).
Reuven

On Fri, Oct 21, 2011 at 8:31 PM, Garcia, Rigo (GSFC-300.0)[MANTECH SRS
TECHNOLOGIES] <[log in to unmask]> wrote:

> Hi everybody,
>
> Does anybody know how do we determine the Maximum Acceptable Moisture
> Content (MAMC) for a board?
>
> I understand that IPC-1601 states that for most designs a MAMC between
0.1%
> and 0.5% of moisture weight to resin weight is adequate. However, it does
> not describe the basis to establish the range. I can think of many
variables
> that can affect this number like minimum pitch, voltage across, component
> clearance, whether the board gets conformal coating or not, etc. I would
> like to know if anybody knows of a safe method to determine the MAMC for a
> given board.
>
> Paul... I can already see your "it depends" coming... :)!
>
> Thanks for the help!
>
> Rigo Garcia
>
> Sr. Quality Assurance Engineer
> Workmanship Standards, Code 300
> NASA, Goddard Space Flight Center
> Greenbelt, MD  20771
> Phone. (301) 286-6129
> Fax.       (301) 286-6576
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>



-- 

Best Regards,

*Reuven Rokah*

Mobile: 972-52-60-120-18
Tele-fax: 97239360688
<http://www.rokah-technologies.com/>[log in to unmask]
[log in to unmask]
www.rokah-technologies.com

**
This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please inform
me by e-mail, phone or fax, and then please delete all of the original files
and all other copies exist.


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2