Hi,
We have a 12L PCB which has 1 additional NPTH (of diameter 0.9mm)
drilled in common ground area. As per the design, this NPTH was
not supposed to be there and hence there is no clearance
in ILs around this NPTH.
The affected PCBs have passed the BBT that was done using the
net list generated from the customer data.
This PCB should comply to IPC 6012, Class 2 requirements.
Please give your inputs if this extra NPTH could cause any functional / reliability
issues and any precautions to be taken if these PCBs were to be used.
Thanks in advance!
Regards,
U.Nagaraj
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|