Doug,
Triboelectric means adding or stealing electrons through friction. How can a
uncured glue (liquid with a high viscosity) move electrons from your nozzle?
I've been in the game for decades and not heard about such things. I've
participated in p-p courses, glue courses, read lots of articles etc, but
missed what you insist.
Human and dry hair has a molecular crystal-like surface, and via the Fermi
level you can move electrons from the orbit. However, if your hair is fat,
there will be no charge movements, because the fat has no specific surface
for that purpose. Likewise, I thought uncured glues were no aspirants
either.
Well, never too late to learn something new.
Inge
Relationship between *triboelectric* charging and surface *...*
<http://search.mywebsearch.com/mywebsearch/redirect.jhtml?qid=62bac059e5f09cb4c1291b201f0024f4&searchfor=kinetic+explanation+of+triboelectric+charges&action=pick&pn=1&n=77decd8b&ptb=naCNCR5Azm75RkmBmXss1w&ptnrS=ZRxdm784YYSE&ss=&st=hp&cb=ZR&pg=GGmain&ord=4&tpr=hpsb&redirect=mPWsrdz9heamc8iHEhldEWVlFOy8LXVdR6PzojpERxbLlEmRQOowS8Qj5BmJGVqQkswtwN%2FH7EAkxVp0REdxDZ8QU9G9gHdhVQrRQ2vn%2FnU%3D&ct=AR>
bleaching, and oxidative dyeing has only a small effect on
*triboelectric*charging. Measurements of the
*kinetics* of *charge* decay indicate that none of these *...*
http://journal.scconline.org/pdf/cc1985/cc036n03/p00189-p00212.pdf -
Cached<http://search.mywebsearch.com/mywebsearch/redirect.jhtml?redirect=GGcached.jhtml&action=click&searchfor=kinetic%2Bexplanation%2Bof%2Btriboelectric%2Bcharges&curl=http%3A%2F%2Fjournal.scconline.org%2Fpdf%2Fcc1985%2Fcc036n03%2Fp00189-p00212.pdf&isDirResults=false&tpr=hpsb&cid=KYJrE_TQtsAJ&ptnrS=ZRxdm784YYSE&st=hp&ptb=naCNCR5Azm75RkmBmXss1w&ct=GC&pg=GGmain&n=77decd8b>
On 13 September 2011 20:06, Douglas Pauls <[log in to unmask]>wrote:
> The coating is insulative in its liquid state as well.
>
> Doug Pauls
>
>
>
> "Mike Fenner" <[log in to unmask]>
> 09/13/2011 12:48 PM
> Please respond to
> <[log in to unmask]>
>
>
> To
> "'TechNet E-Mail Forum'" <[log in to unmask]>, <[log in to unmask]>
> cc
>
> Subject
> RE: [TN] Pneumatic Syringes and ESD
>
>
>
>
>
>
> You would have to check with supplier, or verify it yourself; but though
> the
> coating is insulating when cured it may well not be uncured in liquid
> form.
>
> Regards
>
> Mike
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
> Sent: Tuesday, September 13, 2011 4:53 PM
> To: [log in to unmask]
> Subject: [TN] Pneumatic Syringes and ESD
>
> Good morning all,
>
> Time for a silly question. The question has been raised internally as to
> the risk of ESD generation when an acrylic conformal coating (an
> insulative material) is applied using pneumatic syringes (also an
> insulative material), through a nylon brush (a third synthetic material).
>
> 1. Do you know of any studies done benchmarking static generation levels?
>
> We have done some here, but want to do a sanity check.
> 2. If you have such devices in your facilities, what are your mitigation
> efforts? Air ionizers, grounded tubes?
> 3. Does anyone use, and can recommend, ESD safe syringe bodies and caps?
>
> Many thanks in advance.
>
> Doug Pauls
> Rockwell Collins
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|