In a nut shell: By starting with the thick copper you create fairly
rigid, plated, "solderable" finger(s) / pins, typically at the end of
the circuit. The rest of the flex is etched down in order to make the
cable flexible.
Michael Floyd
CAD/CAM Engineer
Office Address:
4393 Digital Way
Mason, Ohio 45040
Shipping Address:
4240 Irwin Simpson Rd
Mason, Ohio 45040
513-204-7647 (Direct)
513-204-7600 (Main)
513-204-8999 (Main Fax)
[log in to unmask]
www.L-3Com.com/Nova
Mon-Fri, 7:00 AM to 4:30 PM,
alternating Friday's off
(9/80 work system)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly
Sent: Thursday, September 29, 2011 12:58 PM
To: [log in to unmask]
Subject: Re: [TN] Flex Board house
You can look on our website www.pfcflex.com - basically you start with
thick copper and etch so you have thick copper in some areas and thinner
in others - invented in the early 80's. Steve Kelly
Steve Kelly
O (416) 750-8433
C (416) 577-8433
----- Original Message -----
From: Phil Bavaro [mailto:[log in to unmask]]
Sent: Thursday, September 29, 2011 12:53 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Flex Board house
Ok, I will bite.
Could someone please explain to me what a sculptured flex circuit is?
Thanks in advance
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Thursday, September 29, 2011 8:35 AM
To: [log in to unmask]
Subject: Re: [TN] Flex Board house
Craig,
We at AEI has developed a process that is approved and used in Missile
Defense (LMCO).
Rashesh
818-768-3919
_www.accueng.com_ (http://www.accueng.com)
In a message dated 9/29/2011 5:26:09 A.M. Pacific Daylight Time,
[log in to unmask] writes:
Can anyone recommend a flex board house that can do a sculptured
circuit?
Most places I have used before won't even quote it.
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480
F: 607.266.0482
[log in to unmask]<mailto:[log in to unmask]>
P Please consider the environment before printing this e-mail.
________________________________
Confidentiality Notice:
This e-mail contains privileged and confidential information which is
the
property of MPL Incorporated, intended only for the use of the intended
recipient(s). Unauthorized use or disclosure of this information is
prohibited. If you are not an intended recipient, please immediately
notify MPL
Incorporated and destroy any copies of this email. Receipt of this
e-mail shall
not be deemed a waiver by MPL Incorporated of any privilege or the
confidential nature of the information.
Export Control:
This message is intended only for the addressee and may contain
information that is company confidential or privileged. Any technical
data in this
message may be exported only in accordance with the U.S. International
Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export
Administration
Regulations (15 CFR Parts 730-774). Unauthorized use is strictly
prohibited
and may be unlawful. If you are not the intended recipient, or the
person
responsible for delivering to the intended recipient, you should not
read,
copy, disclose or otherwise use this message. If you have received this
email in error, please delete it, and advise the sender immediately.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
------
This message and any attachments are solely for the use of the addressee
and may contain L-3 proprietary information that may also be defined as
USG export controlled technical data. If you are not the intended
recipient, any disclosure, use or distribution of its content is
prohibited. Please notify the sender by reply e-mail and immediately
delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|