http://parts.digikey.com/1/parts/1615283-d-sub-9pos-male-dust-cover-l17d4k63010.html
*Inge*
On 22 September 2011 20:52, Reuven Rokah <[log in to unmask]> wrote:
> If the plastic / connector is antistatic, It should have small amount of
> conductivity. You will have leakage between the connector pins or low
> voltage breakdown.
> Reuven
>
> On Thu, Sep 22, 2011 at 9:19 PM, Dominic Boudreau <
> [log in to unmask]> wrote:
>
> > Hi all, I would like to request your help. We would need to have dust
> > covers for DB type connectors that would be antistatic and that resist at
> > least 150 degrees C. I have searched for off-the-shelf products but I
> don't
> > think it exists. The dust covers that I've found do not resist these
> high
> > temperatures. The other option that we have evaluated would be to make
> these
> > covers by ourselves with a mold. Regarding that, here are my two
> questions:
> >
> > 1) Does anyone know a type of material that would be high temp and
> > antistatic that we could mold easily with a fixture?
> >
> > 2) Is there dust covers that are high temp resistant?
> >
> > Regards
> >
> >
> >
> > Dominic Boudreau
> >
> > Email:[log in to unmask]<mailto:
> > [log in to unmask]>
> >
> >
> > ______________________________________________________________________
> > This email has been scanned by the MessageLabs Email Security System.
> > For more information please contact helpdesk at x2960 or
> [log in to unmask]
> > ______________________________________________________________________
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 16.0
> > To unsubscribe, send a message to [log in to unmask] with following text
> in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> > For additional information, or contact Keach Sasamori at [log in to unmask]
> > 847-615-7100 ext.2815
> > -----------------------------------------------------
> >
>
>
>
> --
>
> Best Regards,
>
> *Reuven Rokah*
>
> Mobile: 972-52-60-120-18
> Tele-fax: 97239360688
> <http://www.rokah-technologies.com/>[log in to unmask]
> [log in to unmask]
> www.rokah-technologies.com
>
> **
> This e-mail message is intended for the recipient only and contains
> information which is CONFIDENTIAL and which may be proprietary of Rokah
> Technologies. If you have received this transmission in error, please
> inform
> me by e-mail, phone or fax, and then please delete all of the original
> files
> and all other copies exist.
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|