Ignorance alert!
What is an XRF measurement, and how do I get one?
Thanks,
Carl
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.
Sent: Monday, September 19, 2011 1:54 PM
To: [log in to unmask]
Subject: Re: [TN] large parts falling off finished surface mount board
assemblies
Carl,
Do not scrap the pad or do any heating or mechanical testing of the
surface where the component fell off. Simply do an XRF measurement of
the pad surface and see what is left. You can also do an XRF
measurement on the component surface. That should give you a first
order approximation of what the problem is. My guess is the gold is
probably completely dissolved in the solder and the solder is on the
component and the failure is at the nickel-tin ICM interface.
Regards,
George
George M. Wenger
Senior Principal Reliability / FMA Engineer Andrew Corporation -
Wireless Network Solutions
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 Office (732) 309-8964 Mobile
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl VanWormer
Sent: Monday, September 19, 2011 3:48 PM
To: [log in to unmask]
Subject: [TN] large parts falling off finished surface mount board
assemblies
A surface mount PC board assembly (made by a local assembly house and
passed by our outgoing test) was returned from the end user, along with
an electrolytic capacitor that they had "knocked off" the board. After
looking at the assembly and component under a microscope, I noticed that
the "gold plated" PC board (Lead free) had a fine granular solder
appearance (much smaller grain than solder paste balls) on the pads
newly exposed, with the whole "melted solder" blobs (in the shape of the
pads) attached to the capacitor leads (with a similar granular
appearance). After minor scraping of various parts, I had come to no
brilliant conclusions, so I pressed my finger nail against an inductor
that was of similar size to the capacitor. It popped off the board with
the same symptoms as the capacitor. After recovering from my surprise,
I realized that I have no clue about the causes or cures for my
component adhesion problem. Can any of the more experienced members of
this fine group direct me to some key words that might lead me to a
quick education (and solution)?
Thanks,
Carl
Carl Van Wormer, P.E., AE7GD
Senior Hardware Engineer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR 97006
Cipher Systems (503) 617-7447 x 5163
Direct Line (503) 425-5163
[log in to unmask] <mailto:[log in to unmask]>
This message may contain confidential and/or proprietary information,
and is intended for the person/entity to whom it was originally
addressed. Any use by others is strictly prohibited. If I sent this to
you by mistake, please be nice and delete it, then tell me of my mistake
so I can send it to the right person.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|