No, ENIG is still a daily pain in the rear. I am dealing with it (not at GD) at different clients almost daily.
Although I am sure it has gotten much better as the board fabricators learn more, and start getting their processes under control, which is the key.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Thursday, September 15, 2011 4:28 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG versus LFHASL
no RF... and no bananas ...
the bad reputation of ENIG, does it not belong to history now? I used to
get ENIG issues on my desk once a week, but have not heard of any problems
for years. Probable cause is that they buy lots and that there is a
stringent quality/process control, not only in a bunch of papers,* but in
the daily routines.* Our purchaser or the component guy knows that he can't
sit in his chair all day, but got to visit the board maker frequently. A
ticket to Shanghai or Tokyo or like costs less than a handful of PWBs.
Don't tell me that your company is a small one, then the reason for personal
contacts is even more worthful. Standing still one week can be catastrophic
for a small entrepeneur with only one source and only one product, while a
mega one can redirigate to another plant in the country or abroad.
I've heard that american electronic engineers in general are little slow
when it comes to 'benchmarking' , but I do not know if it's true.
//Inge
On 15 September 2011 22:40, Phil Nutting <[log in to unmask]> wrote:
> Ok, so we use SMT and PTH circuit boards, all are low speed (20 kHz to 50
> kHz), no BGAs, smallest parts are typically 0603, no Bluetooth, no RF,
> typically 0.015 pitch. Environment might be a medical office, airport,
> semiconductor fab or research lab.
>
> As for all the geniuses getting together to decide... I'm it. There is no
> one else that has in depth knowledge of all the possible factors. I guess
> I could go out to lunch and discuss it with myself over a couple of
> martinis. Yum!
>
> Phil
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> Sent: Thursday, September 15, 2011 3:19 PM
> To: [log in to unmask]
> Subject: Re: [TN] ENIG versus LFHASL
>
> Regarding my previous post, I am not saying anyone should not use ENIG. You
> just need to be knowledgeable in ALL surface finishes before you make a
> selection.
> Surface finish is not something you pull out of your hat based just on
> whether the CCA is going to be lead-free, although that is definitely one of
> the factors.
> For example, you need to consider the type of circuitry. If it is an
> analog, high RF, Bluetooth CCA for example, ENIG would be your last choice
> (it may be too lossy, and if you do not understand what that means you
> should not be determining the surface finish alone).
>
> If it is a double sided SMT CCA with BGAs on both sides, with through-hole
> parts that require hand soldering, and must be processed using lead-free
> solder, why then, ENIG might just be the best choice. Or it might not. In
> that case, OSP is definitely not the best choice.
>
> Selection of finish should be left to a team of engineers who know all of
> the advantages/disadvantages of each finish and understands (intimately)
> his/her particular circuit design types (RF receiver/converter, digital
> processor card, power supply card, D/A card, thermoswitch device, etc,) and
> there are many to consider. The designer, process engineer, and quality
> engineer should also be familiar with the fabrication capabilities (or
> conversely, the weaknesses) of the different fabricators they have a
> business relationship with, and have that in mind when selecting a finish
> also.
>
> It is definitely NOT something a manufacturing engineer alone should decide
> based solely on process type or "personal favorite".
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> Sent: Thursday, September 15, 2011 1:37 PM
> To: [log in to unmask]
> Subject: Re: [TN] ENIG versus LFHASL
>
> In fact, Werner wrote entire papers about the possible problems with using
> ENIG. Here are some;
> http://content.yudu.com/Library/A1qwqg/GlobalSMTampPackagin/resources/61.htm
>
> http://www.trafalgar2.com/documents/Issue_Archive/global_7.3_us_opt.pdf
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Reuven Rokah
> Sent: Thursday, September 15, 2011 1:19 PM
> To: [log in to unmask]
> Subject: Re: [TN] ENIG versus LFHASL
>
> I am in favor of LFHASL because of its robust in processes and storage
> conditions. You just have to choose the right alloy in the HASL process.
>
> You can search in the IPC archive and read Werner recommendations, he was
> favor of Immersion Silver and against ENIG because of the Ni3Sn4 IMC layer,
> High thermal energy (15 degC) at reflow soldering, lnferior electrical
> properties of solder joints and other reasons such solder d black pads.
>
> Reuven
>
> On Thu, Sep 15, 2011 at 8:00 PM, Phil Nutting <[log in to unmask]
> >wrote:
>
> > Hello Technetters,
> >
> > We are having a discussion about the merits of both ENIG and LFHASL.
> > In
> > 2006 when we switch to a RoHS compliant process we evaluated many
> > board finishes and decided, for our volumes, that although ENIG was
> > more expensive it was more robust. LFHASL wasn't ready for prime
> > time, Immersion Silver was great but required careful storage and
> > handling, OSP was not something that fit our process.
> >
> > Now that LFHASL appears to be more main stream we are reconsidering it.
> > ENIG is not always done in-house at some of our fab shops, so that
> > adds time and money to the delivery. These shops now have LFHASL
> > in-house, so there is a potential for some savings here. We have been
> > given stories of storage issues with LFHASL and other concerns too.
> >
> > As I recall, the industry recommended method of storage of bare
> > circuit boards is in a sealed bag with desiccant, regardless of board
> finish.
> > Leaving bare boards unwrapped and in an open bin is just plain bad
> > practice especially if near the ocean.
> >
> > Several of us here think LFHASL is now right for our processes.
> >
> > Please advise if we are off base.
> >
> > Phil Nutting
> > Design for Manufacturing Engineer
> > Kaiser Systems, Inc.
> > 126 Sohier Road
> > Beverly, MA 01915
> > Phone: 978-922-9300 x1310
> > Fax: 978-922-8374
> > e-mail: [log in to unmask]<mailto:[log in to unmask]>
> > www.kaisersystems.com<http://www.kaisersystems.com>
> > www.linkedin.com/in/philnutting<http://www.linkedin.com/in/philnutting
> > >
> >
> >
> > ________________________________
> > Note: All the information contained in this e-mail and its attachments
> > is proprietary to Kaiser Systems, Inc. and it may not be reproduced
> > without the prior written permission of sender. If you have received
> > this email in error, please immediately return it to sender and delete
> > the copy you received.
> >
> >
> > ______________________________________________________________________
> > This email has been scanned by the MessageLabs Email Security System.
> > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > ______________________________________________________________________
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> > unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> > or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> > per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives For additional information, or
> > contact Keach Sasamori at [log in to unmask] or
> > 847-615-7100 ext.2815
> > -----------------------------------------------------
> >
>
>
>
> --
>
> Best Regards,
>
> *Reuven Rokah*
>
> Mobile: 972-52-60-120-18
> Tele-fax: 97239360688
> <http://www.rokah-technologies.com/>[log in to unmask]
> [log in to unmask]
> www.rokah-technologies.com
>
> **
> This e-mail message is intended for the recipient only and contains
> information which is CONFIDENTIAL and which may be proprietary of Rokah
> Technologies. If you have received this transmission in error, please inform
> me by e-mail, phone or fax, and then please delete all of the original files
> and all other copies exist.
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives For additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives For additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives For additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|