TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Thayer, Wayne - IIW" <[log in to unmask]>
Date:
Wed, 7 Sep 2011 16:21:01 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (155 lines)
Hi Wayne - the molten solder interacts with the organic "plug" material 
resulting in outgassing that causes random, nonpredictable voiding which 
can be problematic in some designs.

Dave



"Thayer, Wayne - IIW" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
09/07/2011 03:48 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Thayer, Wayne - IIW" <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
Re: [TN] QFN with solder slug






Has anyone tried just plugging without overplating?  It is so little area 
that I can't imagine the lost soldering surface area will mean anything 
and it should be a lot cheaper and faster to plug than "vippo".

Wayne

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Friday, September 02, 2011 4:10 PM
To: [log in to unmask]
Subject: Re: [TN] QFN with solder slug

Julie,

 What size vias are you filling and capping? You mention these are vias in 
pads, I would guess these are fairly small vias.

 Do you have a picture of one of your QFN locations where you have used 
this process?

Thanks,
Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk
Sent: Friday, September 02, 2011 1:48 PM
To: [log in to unmask]
Subject: Re: [TN] QFN with solder slug

We use a lot of QFNs, and manufacture some for our own use.  We have 
stopped using open vias -- no matter what the manufacturer says, the 
soldering is inconsistent and adding solder to compensate for wicking away 
can lead to the other issue of the ground pad lifting the part and causing 
opens.  Overprinting the groundpad (or pinpads) can also lead to 
connection between ground pad and pin pad solder and siphoning of the pin 
pad solder into the groundpad joint, causing opens.  We use the fill with 
epoxy and cap plate over method (which we call vippo, via in pad plated 
over).  This adds to the cost of the board because there are additional 
drilling and plating steps, but we get consistent results, better quality 
and the heat transfer is better.  We don't plate-shut , which I would 
guess is pretty specialized and expensive for thru vias.  Dave's followup 
sounded more like vippo.   We never use the cap one side method.  We have 
reliability concerns with trapping acids in this blind hole.  The issue 
with voids is another good one.  Definitely fewer voids with the vippo 
method, but it can still be a problem.  Optimization of the paste pattern 
and process help.  We have not tried the design to vent via diagonal 
solder mask presenting in a paper at IPC2011.    --Julie



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To 
unsubscribe, send a message to [log in to unmask] with following text in the 
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: 
send e-mail to [log in to unmask]: SET Technet Digest Search the archives of 
previous posts at: http://listserv.ipc.org/archives For additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are 
intended solely for the use of the individual or entity to whom they are 
addressed. If you have received this e-mail in error please notify the 
sender.
Please note that any views or opinions presented in this e-mail are solely 
those of the author and do not necessarily represent those of ITT 
Corporation. The recipient should check this e-mail and any attachments 
for the presence of viruses. ITT accepts no liability for any damage 
caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2