Wire splay is a defect for Class 2 and 3 (ref IPC-A-610D, sec 6.9.1). I do not have a handy cope of Rev E to see if the section is the same...
-----Original Message-----
From: Goodyear, Patrick [mailto:[log in to unmask]]
Sent: Tuesday, September 20, 2011 2:04 PM
To: [log in to unmask]
Subject: Re: [TN] Birdcaging
Typically birdcaging is at the junction of the lead and the insulation with separation of the strands there. I looks like the lead was improperly tinned before it was wrapped around the turret. I would say it would be minimum acceptable.
Pat
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Juan T. Marugan
Sent: Tuesday, September 20, 2011 10:04 AM
To: [log in to unmask]
Subject: [TN] Birdcaging
I'd like to know if the strand separation at the end of the wrap is birdcaging, that is, if it is a defect condition. I attach the link of the photo:
http://ipc-technet.groupsite.com/galleries/photo/216475
Thank yo so much,
Juan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|