TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Cedric ORAIN <[log in to unmask]>
Date:
Wed, 14 Sep 2011 14:43:48 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Message-ID:
<001301cc730e$3dc32f80$b9498e80$@com>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<04db01cc72f7$90d77670$b2866350$@[log in to unmask]>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (176 lines)
It is a really complicated problem Cedric.

If the board has been fluxed with a combination of agents and carriers the
result can be very difficult to remove.
So, the cleaning process might not provide the results needed to prevent
electrochemical migration, even a solvent cleaning process.

And no, the methods commonly used to measure ionic contamination are not
assurance that your cleaning process is adequate, especially when fluxing
agents have been mixed without regard for the subsequent cleaning process.
Here I am speaking of the various R.O.S.E. test results. They are best used
to verify that your validated cleaning process has not changed. 

Guy




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cedric ORAIN
Sent: Wednesday, September 14, 2011 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] Flux Compatibility

Do you agree that in case fluxes interact badly we can prevent
SIR/electromigration issue by cleaning the board ?

Perhaps it wasn't clear on my email but these products are 100% cleaned
(solvent process). 

So we should just have to check that the cleaning process is efficient
measuring ionic contamination, don't we ?

Regards,

Cedric 

-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Karen Tellefsen
Envoyé : mercredi 14 septembre 2011 15:05
À : [log in to unmask]
Objet : Re: [TN] Flux Compatibility

Some flux materials don't play well with others, possibly resulting in low
SIR and Electrochemical migration., and compatibility testing helps to
ensure that combinations of materials work well together.  I test many
combinations of Alpha materials for SIR and ECM.  So do Kester and Indiujm
for their respective materials,  The compatibility testing may have already
been done by your paste and flux supplier; ask them if they have data.

Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069



                                                                            
                                                                            
                                                                            
   [TN] Flux Compatibility                                                  
                                                                            
                                                                            
   Cedric ORAIN                                                             
                 to:                                                        
                   TechNet                                                  
                                                        09/14/2011 03:10 AM 
                                                                            
                                                                            
                                                                            
                                                                            
   Sent by:                                                                 
          TechNet <[log in to unmask]>                                         
   Please respond to TechNet E-Mail Forum, Cedric ORAIN                     
                                                                            
                                                                            
                                                                            






Good morning dear Technetters,

I'm asked by one of my customer if I checked the compatibility between in
one hand the no-clean flux from the SMD paste and the other hand the resin
flux from the wires.

The answser was no !

Could you advise which kind of issue could occur if any ?

Thanks for your help,

Regards,

Cedric
www.inovelec-groupe.com




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2