I didn't mean that I could peel the solder off the leads, but that I could shave it off with my knife blade, indicating that all the solder went with the component and none was left on the PC board pads.
Later,
Carl
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Tuesday, September 20, 2011 9:23 AM
To: [log in to unmask]
Subject: Re: [TN] large parts falling off finished surface mount board assemblies
Interesting that you could also peel the solder off the leads. Adds to the reflow process failure idea.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------