TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Thu, 29 Sep 2011 17:54:15 +0000
Reply-To:
Message-ID:
Subject:
From:
vladimir Igoshev <[log in to unmask]>
Content-Type:
text/plain
In-Reply-To:
Content-Transfer-Encoding:
base64
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
It doesn't make much sense at least to me, as the boards go back to normal after second re-flow. Once cured, epoxy can not go back!!!!
Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

-----Original Message-----
From: Joyce Koo <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Thu, 29 Sep 2011 13:47:19 
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject: Re: [TN] Board question

Did you check the degree of cure of the pcb?  (or delta Tg of incoming pcb, (1st scan - 2nd scan) using either TMA or DSC?  If less than 5C, the stuff is properly cured.. Otherwise, it is not).  My 2 cents. 
            jk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev. PhD
Sent: Thursday, September 29, 2011 12:50 PM
To: [log in to unmask]
Subject: [TN] Board question

Hi TechNetters,

I have a question for board gurus, as I'm almost lost.

Here is a story. A panel of four simple 4 layers FR4 twists after
going through the first side re-flow and flatten out after the second
side is re-flowed.   It does the same thing with and without the
components placed.

The panels are from  new vendor and the old ones had never exhibited
the problem. What confused me is that both boards (from both of the
vendors) were built identically: dielectric layers and  Cu
layers are look identical thickness- wise.

There are no signs of resin recession or delamination in
cross-sections which could have pointed out at incomplete curing.

Glass bundles look also identical.

What else it could be?

Any suggestions are deeply appreciated.
-- 
Best regards,

Vladimir Igoshev. PhD                          mailto:[log in to unmask]

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 16.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2