TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 29 Sep 2011 16:04:59 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Temkin, Gregg" <[log in to unmask]>
Message-ID:
Subject:
From:
"Temkin, Gregg" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (78 lines)
Appendix C looks like the ticket.  Thanks very much.  -  Gregg

From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, September 29, 2011 8:34 AM
To: TechNet E-Mail Forum; Temkin, Gregg
Subject: Re: [TN] "Compatibility" testing of fluxes


Greg, everything is an "it depends" situation.

There are many different ways in which material and process compatiblity can be demonstrated.  Two widely accepted methods are to use J-STD-001D, Appendix C, or to use the new IPC-9202 protocol.  Both are available from the IPC.  The 9202 is being printed now and should be available any day now.  It just passed ballot earlier this month.  I hope to have the companion IPC-9203 document, which explains 9202, done by the end of the year.  Then I may launch into IPC-9204, which explains the 9203.  Maybe not.

Doug Pauls

"Temkin, Gregg" <[log in to unmask]<mailto:[log in to unmask]>>
Sent by: TechNet <[log in to unmask]<mailto:[log in to unmask]>>

09/29/2011 10:19 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]<mailto:[log in to unmask]>>; Please respond to
"Temkin, Gregg" <[log in to unmask]<mailto:[log in to unmask]>>


To

<[log in to unmask]<mailto:[log in to unmask]>>

cc

Subject

[TN] "Compatibility" testing of fluxes







J-STD-001 states that fluxes with activity levels of L0 and L1 shall be used but other fluxes with other activity levels may be used as long as data is available "demonstrating compatibility".  Are there any standard "compatibility" tests or is this another one of those "it depends" situations.


Gregg Temkin
Principal Manufacturing Engineer
(425) 376-4429
[Description: Description: clip_image002]


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2