TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Date:
Tue, 27 Sep 2011 12:51:10 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Amol Kane <[log in to unmask]>
Message-ID:
<C23267C3AF7B4842B685FC757EE8A7B8533AA772B0@catvesexch01>
Subject:
From:
Amol Kane <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
base64
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Leland,
After going thru the technet archives, talking to our paste manufacturers, and reading their SOPs for paste handling, we concluded that 7 days at RT was the usable limit (as long as the paste tube/tub is sealed). We have been using that time limit with no paste issues.

How did you arrive at the 3 days? (experimentation, past experience etc?). what I am getting is that there may be no need to re-certify after 3 days


Regards,
Amol Kane | Process Engineer
Catalyst Manufacturing Services, Inc.
941 Route 38, Owego NY 13827
Phone: (607) 687-7669 Extn 349 | Website: www.catalystems.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Tuesday, September 27, 2011 11:42 AM
To: [log in to unmask]
Subject: [TN] Solder Paste Shelf Life Extension

Folks,

Quick question here...

We have a rule here to scrap solder paste after it's been out of the fridge for 3 days.  If we recertify and extend the expiration date by first verifying the proper viscosity, is it permissible to return the paste to the jar that was used for the viscosity testing?

Thanks for your help,

Leland

________________________________

“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 16.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2