TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Sat, 17 Sep 2011 20:27:17 +0100
Reply-To:
Message-ID:
<20F332E306644764A6C272DA039FC053@MikeLaptop>
Content-Transfer-Encoding:
7bit
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
BSAP
MIME-Version:
1.0
Parts/Attachments:
text/plain (124 lines)
My 2 cents
No clean fluxes work in different ways, thus (oversimplifying) high solids
rosin based fluxes work by encapsulating ionics and low solids by
inactivating. If you use a low solids flux with a rosin material, you're
thinking flux but chemically what you are doing is adding dirty solvent (IPA
with 1,2,3% whatever ionics) to the rosin. This will tend to
dissolve/disperse and contaminate it, overloading the rosin and reducing its
encapsulation effectiveness. It may be that keeping to the same basic flux
formulation types irrespective of supplier works out OK, but the world is
not oversimplified so it may not. If using multiple fluxes therefore it is
not a good idea to also mix suppliers - at least without testing. If there
are problems a single supplier will know what is being mixed and make
recommendations and is likely to have tested recommended combinations.
Conversely he clearly can not know the formulation details of all other
supplier products and certainly not how multiple different supplier products
will interact with each other and his own material.

Regards

Mike 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, September 15, 2011 1:46 AM
To: [log in to unmask]
Subject: Re: [TN] Flux Compatibility

Cedric,
In some rather rare cases fluxes of different types (core wire vs. solder
paste, wave flux vs. solder paste, etc.) when mixed together fail SIR and/or
electrochemical migration testing, even though they individually pass.  I
can't prove it, but I would expect that a failure would be more likely to
happen if the two materials are not made by the same supplier.

That being said, even large companies like Nortel (now deceased  :( ) did
NOT test ever combo, not even 10% of the combinations, because, frankly, it
would be too costly and the risk was deemed low enough to live with the
possibility.

So there is some risk, but as far as I know, no one in our industry has ever
quantified what that risk is.

Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cedric ORAIN
Sent: Wednesday, September 14, 2011 3:10 AM
To: [log in to unmask]
Subject: [TN] Flux Compatibility

Good morning dear Technetters,

I'm asked by one of my customer if I checked the compatibility between in
one hand the no-clean flux from the SMD paste and the other hand the resin
flux from the wires.

The answser was no !

Could you advise which kind of issue could occur if any ?

Thanks for your help,

Regards,

Cedric
www.inovelec-groupe.com




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2