Thanks Rudy.
> Date: Fri, 5 Aug 2011 23:54:03 -0700
> From: [log in to unmask]
> Subject: Re: [TN] Removing SnCl2
> To: [log in to unmask]
>
> Gerry:
> Do not know specific compound, but laminate is highly reactive, and particularly if you have brominated laminate, the bromine forms unstable bonds.
>
> Rudy Sedlak
>
> --- On Fri, 8/5/11, Gerry Gagnon <[log in to unmask]> wrote:
>
> From: Gerry Gagnon <[log in to unmask]>
> Subject: Re: [TN] Removing SnCl2
> To: [log in to unmask]
> Date: Friday, August 5, 2011, 9:30 AM
>
>
>
> Rudy,
>
>
>
> Thanks! Would you happen to know what the SN+2 binds with in the laminate to form the organo-metallic compound?
>
>
>
> Gerry
>
>
>
>
>
>
>
>
> ----------------------------------------
> > Date: Thu, 4 Aug 2011 12:37:46 -0700
> > From: [log in to unmask]
> > Subject: Re: [TN] Removing SnCl2
> > To: [log in to unmask]
> >
> > Gerry: If the Tin is introduced to the surface as Sn+2, and reacts with say laminate, to form an organo-metallic, and then becomes oxidized to Sn+4, it takes an act of divine intervention to remove it, OR strong caustic, OR HF, + some temperature.
> > When a Tin stripper works, it dissolves the Tin as Sn+2, which is subsequently, and rapidly oxidized to Sn+4, probably by atmospheric Oxygen. So, when stripping, there will be some Sn+2, and a lot of Sn+4 around.
> >
> > Rudy Sedlak
> >
> > --- On Thu, 8/4/11, Gerry Gagnon <[log in to unmask]> wrote:
> >
> > From: Gerry Gagnon <[log in to unmask]>
> > Subject: Re: [TN] Removing SnCl2
> > To: [log in to unmask]
> > Date: Thursday, August 4, 2011, 11:05 AM
> >
> > Hi Rudy, This is what I thought when I saw your original response. What troubles me is how the tin can persist through all the pre-mask preparation (pumice plus microetch), mask rinses, surface finish preparation/deposition/rinses, and final board wash (if any). The SN+4 must be pretty tenacious. Gerry
> > > Date: Thu, 4 Aug 2011 10:16:23 -0700
> > > From: [log in to unmask]
> > > Subject: Re: [TN] Removing SnCl2
> > > To: [log in to unmask]
> > >
> > > See below please...
> > >
> > > --- On Thu, 8/4/11, Brian Ellis <[log in to unmask]> wrote:
> > >
> > > From: Brian Ellis <[log in to unmask]>
> > > Subject: Re: [TN] Removing SnCl2
> > > To: [log in to unmask]
> > > Date: Thursday, August 4, 2011, 8:16 AM
> > >
> > > Logically, I would expect no Sn on a bare ENIG board. Where would it
> > > come from?
> > >
> > > From Tin plating as etch resist. Tin strippers have Sn+4 dispersed in solution, which is why they look milky.
> > > Rudy Sedlak
> > >
> > > The only answer I can offer is from the copper treatment.
> > > When I was half my present age (~1970), I seem to remember Gould (?)
> > > offered a copper treated with brass; I thought this had died a natural
> > > death (peel strength?) but has someone resurrected it??? If so, then
> > > using a chloride etchant would be a natural source.
> > >
> > > Brian
> > >
> > > On 04/08/2011 15:22, Don McFarland wrote:
> > > > Sn(iv) would make more sense because this stuff seems impervious to anything we've thrown at it.
> > > >
> > > > We have traced it back and found that this residue is visually present on the bare ENIG pcb. We have the sem, edx ad ftir tests being done on the bare board to compare residual signature to post-assembly residues. The interesting this was our FTIR only showed FR-4, but nothing else. Should ftir detect these Sn residues if present and adequate sample captured? I am wondering if this is a laminate curing issue and not a contamination issue, since our data points arent seeing the chemistry.
> > > >
> > > > The SEM/edx found minute flakes of Sn that appear to attach to Cu contaminate found on bare pcb. These embedded flakes are only visible at 1000x and are small at that...just a bit out of the allowed mag for fod inspection.
> > > >
> > > >
> > > >
> > > > Sent from my iPhone
> > > >
> > > > On Aug 3, 2011, at 4:24 PM, R Sedlak<[log in to unmask]> wrote:
> > > >
> > > >> Don: I think I qualify as a "real Chemist", or at least I have a lot of people fooled...
> > > >> Actually, SnCl2 is easy to remove, but it is highly unlikely your deposit is SnCl2, but is much more likely to be SnCl4 (Stannic Chloride) which is rather more difficult to remove...
> > > >> I would recommend either a Caustic cleaner, preferably with some chelate, if your substrate can tolerate that.
> > > >> If not, probably the only other cleaner which will remove Stannic Chloride is a dip in an Ammonium Bifluoride solution, say, 5-10%. Stannic salts are highly insoluble, and hydrolyze easily to Stannic oxide, which needs either strong alkali, or HF to remove.
> > > >> Wish I had better news.
> > > >> Rudy Sedlak
> > > >> RD Chemical Company
> > > >>
> > > >> --- On Wed, 8/3/11, Don McFarland<[log in to unmask]> wrote:
> > > >>
> > > >> From: Don McFarland<[log in to unmask]>
> > > >> Subject: [TN] Removing SnCl2
> > > >> To: [log in to unmask]
> > > >> Date: Wednesday, August 3, 2011, 10:49 AM
> > > >>
> > > >> Any ideas on methods to remove a tin chloride residue that was found on a FR-4 substrate after wave solder. We have done some good homework to find the source, but we are looking for good and proven methods to remove the residues from affected assemblies.
> > > >>
> > > >> Any input is welcome.
> > > >>
> > > >> Regards,
> > > >>
> > > >> Don McFarland
> > > >>
> > > >> **********************************
> > > >> CONFIDENTIALITY NOTICE: The information in this electronic mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named above. If the reader of this message is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of the transmission is strictly prohibited. If you have received this transmission in error, delete the message and immediately notify us by telephone at 435.792.4949 or by responding to this email.
> > > >> **********************************
> > > >>
> > > >> ______________________________________________________________________
> > > >> This email has been scanned by the MessageLabs Email Security System.
> > > >> For more information please contact helpdesk at x2960 or [log in to unmask]
> > > >> ______________________________________________________________________
> > > >>
> > > >> ---------------------------------------------------
> > > >> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> > > >> To unsubscribe, send a message to [log in to unmask] with following text in
> > > >> the BODY (NOT the subject field): SIGNOFF Technet
> > > >> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > > >> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > > >> Search the archives of previous posts at: http://listserv.ipc.org/archives
> > > >> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> > > >> -----------------------------------------------------
> > > >
> > > > ______________________________________________________________________
> > > > This email has been scanned by the MessageLabs Email Security System.
> > > > For more information please contact helpdesk at x2960 or [log in to unmask]
> > > > ______________________________________________________________________
> > > >
> > > > ---------------------------------------------------
> > > > Technet Mail List provided as a service by IPC using LISTSERV 16.0
> > > > To unsubscribe, send a message to [log in to unmask] with following text in
> > > > the BODY (NOT the subject field): SIGNOFF Technet
> > > > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > > > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > > > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > > > For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> > > > -----------------------------------------------------
> > > >
> > >
> > > ______________________________________________________________________
> > > This email has been scanned by the MessageLabs Email Security System.
> > > For more information please contact helpdesk at x2960 or [log in to unmask]
> > > ______________________________________________________________________
> > >
> > > ---------------------------------------------------
> > > Technet Mail List provided as a service by IPC using LISTSERV 16.0
> > > To unsubscribe, send a message to [log in to unmask] with following text in
> > > the BODY (NOT the subject field): SIGNOFF Technet
> > > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > > For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> > > -----------------------------------------------------
> > >
> > > ______________________________________________________________________
> > > This email has been scanned by the MessageLabs Email Security System.
> > > For more information please contact helpdesk at x2960 or [log in to unmask]
> > > ______________________________________________________________________
> > >
> > > ---------------------------------------------------
> > > Technet Mail List provided as a service by IPC using LISTSERV 16.0
> > > To unsubscribe, send a message to [log in to unmask] with following text in
> > > the BODY (NOT the subject field): SIGNOFF Technet
> > > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > > For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> > > -----------------------------------------------------
> >
> >
> > ______________________________________________________________________
> > This email has been scanned by the MessageLabs Email Security System.
> > For more information please contact helpdesk at x2960 or [log in to unmask]
> > ______________________________________________________________________
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 16.0
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> > -----------------------------------------------------
> >
> > ______________________________________________________________________
> > This email has been scanned by the MessageLabs Email Security System.
> > For more information please contact helpdesk at x2960 or [log in to unmask]
> > ______________________________________________________________________
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 16.0
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> > -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|