Hi Rex - no, this isn't a Weekly Quiz question but that did give me a
chuckle to start the day! I am working on the revision of the IPC JSTD 002
Solderability specification and need that density value for SAC305 solder
as part of the specification test methods. Bev Christian and Graham
Naisbitt have found the values for Sn63 and Sn60 for me but I/we am still
in search of the SAC305 number. I do need the value to be accurate - where
did ya find the 7280 value?
Dave
"Rex Waygood" <[log in to unmask]>
08/31/2011 07:35 AM
To
"TechNet E-Mail Forum" <[log in to unmask]>, <[log in to unmask]>
cc
Subject
RE: [TN] Solder Data Question
I don't know as I've hunted on the web and cannot find a fact I'd trust.
I assume this isn't a Wednesday Quiz?
From what I've found on the web, I'd say/guess about 7280 kg/m3
How accurate do you need to know the answer?
Regards
Rex
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: 31 August 2011 13:08
To: [log in to unmask]
Subject: [TN] Solder Data Question
Hi folks - does anyone have the density value (kg/m3) for SAC305 at
245C?
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|