Tin Chloride is:
-insoluble in normal industrial solvents
-harmless
/Inge
On 3 August 2011 19:49, Don McFarland <[log in to unmask]> wrote:
> Any ideas on methods to remove a tin chloride residue that was found on a
> FR-4 substrate after wave solder. We have done some good homework to find
> the source, but we are looking for good and proven methods to remove the
> residues from affected assemblies.
>
> Any input is welcome.
>
> Regards,
>
> Don McFarland
>
> **********************************
> CONFIDENTIALITY NOTICE: The information in this electronic mail
> transmission is legally privileged and confidential information intended
> only for the use of the individual or entity named above. If the reader of
> this message is not the intended recipient, you are hereby notified that any
> dissemination, distribution or copying of the transmission is strictly
> prohibited. If you have received this transmission in error, delete the
> message and immediately notify us by telephone at 435.792.4949 or by
> responding to this email.
> **********************************
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|