Frank,
You may also look at some of the rework tools such offered by
circuitmedic.com. They have some clean looking solutions to jumper wires
etc. I use them a lot for PCB repair and I have noticed some of their
rework offerings. I have not used them for anything but PCB repair.
Leif Erik Laerum
On 7/29/2011 5:53 PM, Steve Gregory wrote:
> Hi Frank,
>
> I have your doc posted here:
>
> http://stevezeva.homestead.com/Rework_Instructions.doc
>
> Looks like you're dealing in some tight quarters there, it really
> makes things tough. Doesn't help that there are all of them unmasked
> vias around either. Is the IC a QFN? I don't see any leads coming off
> it. Don't know what the application is, so I can't comment on the
> suitability of this solution. Generally from my experience, the
> customer is the customer, and whatever solution is decided on, both
> the vendor and the customer need to buy into it. and that's where
> having a real partnership with each other makes a huge difference when
> trying to work through situations like this.
>
> Nobody likes to have to resort to such measures as this, but shi...I
> mean stuff, happens.
>
> We've done some crazy things here. One of the latest ones was this:
>
> http://stevezeva.homestead.com/Crazy_Mod_Inst.jpg
>
> These were the instructions from our customer, and in all fairness
> they asked first if we could do this. All we could do is tell them
> that we would try. Take note that these are 0402's. It looked kinda'
> feasible on paper. But what we didn't take into account was that the
> 120nH inductor was a Coilcraft part with bottom only terminations.
> Below is what we wound-up doing:
>
> http://stevezeva.homestead.com/Crazy_Mod_Done.jpg
>
> This is where having good, and I mean good, rework technicians is
> absolutely priceless. I am constantly amazed at what our technicians
> can accomplish. A similar mod had to be done at another location on
> the board, and thank goodness we didn't have to do this on too many
> boards. As far as I know this worked, and our customer was grateful.
>
> Steve
>
>
>
> -----Original Message----- From: Frank Kimmey
> Sent: Friday, July 29, 2011 4:36 PM
> To: [log in to unmask]
> Subject: [TN] Rework from cut and jump
>
> I have asked Steve G to post a rework file for me.
> Our customer seems to dislike the white wire approach.
> Can anyone offer a more elegant solution?
> Please feel free to contact me offline if you are looking for the
> business.
> Any suggestions will be appreciated
> Thanks,
> FNK
>
> Frank N Kimmey CID+
> Manager - PCB Design
> Powerwave Technologies Inc
> Mobile - 916-670-0645
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
CONFIDENTIALITY NOTICE: This email and any attachments are Texas Memory Systems' proprietary material for the exclusive and confidential use of the intended recipient. If you are not the intended recipient, please do not read, distribute or take action in reliance upon this message. Any unauthorized disclosure is prohibited. If you have received this in error, please notify us immediately by return email and promptly delete all copies of this message and its attachments from your computer system.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|