TECHNET Archives

August 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Scott Westheimer <[log in to unmask]>
Date:
Wed, 3 Aug 2011 17:44:11 +0000
Reply-To:
Message-ID:
Subject:
From:
vladimir Igoshev <[log in to unmask]>
Content-Type:
text/plain
In-Reply-To:
Content-Transfer-Encoding:
base64
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Absolutely right. I just wish that all board shops has the same philosophy.
Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

-----Original Message-----
From: Scott Westheimer <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Wed, 3 Aug 2011 13:26:35 
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
        Scott Westheimer <[log in to unmask]>
Subject: Re: [TN] Steps to take to prevent ENIG issues

I would not be so fast to through out the baby with the bath water. Yes there are other alternatives but a shop that controls their process, i.e. turn over's, chemistry concentrations, times, temperatures and such, should be able to provide a good surface finish. ENIG has been around a long time and yes there can be problems with soldering, peeling and solder mask lifting but 9 times of of 10 it is the fabricators lack of control.

Scott B. Westheimer
Account Manager, Rayben PCB
5709 Clarks Fork Drive
Raleigh, NC 27616
[log in to unmask]
Office: +1(919)278-7539
Home: +1 (919)713-0748
Cell NC: +1 (919)800-1876


 



 > Date: Wed, 3 Aug 2011 16:49:34 +0100
> From: [log in to unmask]
> Subject: Re: [TN] Steps to take to prevent ENIG issues
> To: [log in to unmask]
> 
> Agree, don't use ENIG.
> I am in the middle of a protracted ENIG problem which according to the
> manufacturer is down to our processes and their tests of the board show
> them to be perfect.
> However in order to solder 4 power pad QFPs we are having to scrape off
> the gold to get the nickel to solder.
> Our production and a test at NPL shows the ENIG to be very poor.
> ENIG is the pits.
> 
> Regards
> Rex
> 
> 
> 
>  
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.
> Sent: 03 August 2011 16:43
> To: [log in to unmask]
> Subject: Re: [TN] Steps to take to prevent ENIG issues
> 
> The only guarantee is not to use ENIG.  To minimize ENIG issues select a
> good PCB fabricator and make sure they control their process.
> 
> Regards,
> George
> George M. Wenger
> Senior Principal Reliability / FMA Engineer Andrew Corporation -
> Wireless Network Solutions 40 Technology Drive, Warren, NJ 07059
> (908) 546-4531 Office (732) 309-8964 Mobile
> E-mail: [log in to unmask]
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> Sent: Wednesday, August 03, 2011 11:17 AM
> To: [log in to unmask]
> Subject: [TN] Steps to take to prevent ENIG issues
> 
> I have a client who is switching PWB fabricators for ENIG finishes. They
> are fully aware of ENIG issues such as Black Pad, Brittle Nickel, etc.,
> and want to know whatever steps can be taken to prevent ENIG PWBs from
> reaching production with these issues.
> Does anyone have any suggestions?
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives For
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives For
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
 		 	   		  

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 16.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2