TGASIA Archives

August 2011

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Leesha \"Lixia\" PENG" <[log in to unmask]>
Reply To:
Asia Committe Task Group Forum <[log in to unmask]>, Leesha "Lixia" PENG
Date:
Wed, 10 Aug 2011 20:22:34 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
paul,能查到这个人是谁吗?woaini888



Leesha Peng

彭丽霞

IPC中国总经理

18616593891





在 2011-8-11,上午9:02,"woaini888" <[log in to unmask]<mailto:[log in to unmask]>> 写道:



你这板很好焊啊,给我电话啊13924605925



在 2011-08-10 23:39:04,"代华" <[log in to unmask]<mailto:[log in to unmask]>> 写道:

各位前辈:

      我公司最近生产的一款电子产品在波峰焊接的过程中贴片电阻一端不上锡,请问是波峰焊没有调好还是设计不到位?

      如果是波峰焊没有调好,请问波峰焊的参数该怎么设置?

      如果是设计的问题,请问贴片应该怎么调整位置? 谢谢了!非常感谢!











______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]> [log in to unmask]<mailto:[log in to unmask]>

______________________________________________________________________







______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>

______________________________________________________________________


ATOM RSS1 RSS2