I would think LF HASL would be SAC, or a high tin alloy (similar to SN100C). Not pure tin
Amol Kane | Process Engineer
Catalyst Manufacturing Services, Inc.
941 Route 38, Owego NY 13827
Phone: (607) 687-7669 Extn 349 | Website: www.catalystems.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Honsowetz, Eric
Sent: Wednesday, August 10, 2011 8:57 AM
To: [log in to unmask]
Subject: Re: [TN] Lead Free HASL and whiskers
Good Morning Mark,
The classic answer ... it depends ...
Is there an industry standard for Pb-free HASL? IPC does not appear to
have a specification.
The drawing or procurement document might define the material used ...
It would be expected that the HASL would be a common soldering material
which would not be pure Sn.
Pure Sn would probably be a difficult material to use for HASL due to
its tendency to react with Cu.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Woolley, Mark D.
(Mark)
Sent: Tuesday, August 09, 2011 6:19 PM
To: [log in to unmask]
Subject: [TN] Lead Free HASL and whiskers
I have a question now that our company is beginning to use lead free
HASL as a solderability finish. I am seeing a few (<5%) filled vias on
each board I examine. Does anyone know if the manufacturer's are using
pure tin, and if they are has anyone looked at tin whiskers from HASL
filled vias?
Thanks,
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster, CO 80234 USA |
Voice (Lab): (303) 538-2166 | email: [log in to unmask] |
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
**********************
** LEGAL DISCLAIMER **
**********************
This E-mail message and any attachments may contain
legally privileged, confidential or proprietary
information. If you are not the intended recipient(s),
or the employee or agent responsible for delivery of
this message to the intended recipient(s), you are
hereby notified that any dissemination, distribution
or copying of this E-mail message is strictly
prohibited. If you have received this message in
error, please immediately notify the sender and
delete this E-mail message from your computer.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|