No arguments here Eric, but Jim is dealing with an "H" activity flux, and
quite often there may be additional tests required by contract. They vary
from customer to customer, so I asked the question before giving further
advice, as to what was contractually required. IC is very much a more
accurate test and the one to use.
Doug Pauls
"Honsowetz, Eric" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
08/30/2011 03:30 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Honsowetz, Eric" <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
Re: [TN] PWB Cleanliness
It depends however the ROSE test was developed far far away a long long
time ago and if the question is actual cleanliness (verses contractual
cleanliness) IPC has a couple of test standards - IPC-TM-650 2.3.25 &
IPC-650-2.3.28.
The first is for ROSE and the second is Ion chromatography which is more
accurate so I am told.
eric
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Tuesday, August 30, 2011 3:04 PM
To: [log in to unmask]
Subject: Re: [TN] PWB Cleanliness
There you go; back-petaling already.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Tuesday, August 30, 2011 11:58 AM
To: [log in to unmask]
Subject: Re: [TN] PWB Cleanliness
Jim,
There are lots of "it depends" that I could throw at this, but lets
start
with what you are contractually bound to provide. I would expect at
least
the ROSE test. Then we can go from there.
Doug Pauls
"Marsico, James - ES" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
08/30/2011 01:45 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Marsico, James - ES" <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
[TN] PWB Cleanliness
Hello Technet, I know I should know this, but what cleanliness testing
should be performed on CCAs that are soldered with an ORH0 solder paste?
What should the acceptance criteria be prior to conformal coating?
Thanks in advance,
Jim Marsico
ITT Corporation
1500 New Horizons Blvd.
North Amityville, NY 11701
631-630-5079
[log in to unmask]<mailto:[log in to unmask]>
________________________________
This e-mail and any files transmitted with it may be proprietary and are
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this e-mail in error please notify the
sender.
Please note that any views or opinions presented in this e-mail are
solely
those of the author and do not necessarily represent those of ITT
Corporation. The recipient should check this e-mail and any attachments
for the presence of viruses. ITT accepts no liability for any damage
caused by any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
**********************
** LEGAL DISCLAIMER **
**********************
This E-mail message and any attachments may contain
legally privileged, confidential or proprietary
information. If you are not the intended recipient(s),
or the employee or agent responsible for delivery of
this message to the intended recipient(s), you are
hereby notified that any dissemination, distribution
or copying of this E-mail message is strictly
prohibited. If you have received this message in
error, please immediately notify the sender and
delete this E-mail message from your computer.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|