Dear all,
"Simple" question regarding prepreg storage conditions.....
IPC4101 states that prepregs has shelf life of 6 months while in condition 1 at <5 Degrees C (41 F) and 3 months while in condition 2 at <23 Degrees C (73F) and <50% Rh.
Condition 1 does not clearly state a humidity control.
Does Humidity still have to be less than 50% while under condition 1? or is this a given considering Temperature vs. Humidity relationship
rgds
Colin
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------