Hi Victor,
I have your picture posted here:
http://stevezeva.homestead.com/Resistor_Coating.jpg
I would think that if the protective coating encroached onto the end cap on
the top, it shouldn't pose any problem as long as it didn't interfere with
allowing a good solderjoint to form. As far as the other questions, I can't
help much there...it's outside of my realm of knowledge.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Tuesday, July 12, 2011 10:36 AM
To: [log in to unmask]
Subject: [TN] FW: Thin Film Ceramic Resistor, 51K, serpentine
Fellow TechNetters:
I did not receive many responses to mu original inquiry, so I will post
again. I hope someone will contribute or lead to to some solid
information/data/article regarding the process of ceramic thin Film process.
I will post a conceptual photo I what I am searching for with Steve.
Victor,
_____________________________________________
From: Hernandez, Victor G
Sent: Friday, July 01, 2011 9:59 AM
To: TechNet E-Mail Forum
Cc: Hernandez, Victor G
Subject: Thin Film Ceramic Resistor, 51K, serpentine
Fellow TechNetters:
Do anyone out there have experience/knowledge of the ceramic resistor
process and parameter specification? Is there a base material applied
before thin film application? Is there a method/technique for checking
coating integrity. Similar to, Chemical test for passivation pin hole on
ICs. Is there a spec for end cap/wrap around? Etc....
Victor,
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|