Guy,
Some groups/people consider plastic packages to be 'hermetic', but I dare
say
that you would not get individuals which have built true hermetic hybrids to
agree to that.
Same way that some companies advertise 'hermetic' polymers - maybe for days
or weeks, but not for the long haul.
It sounds like they are giving themselves a mighty big CYA in a generic
sense.
Then making it known they have a high rel version as well - for the special
occasions
Maybe they have some history of their epoxy to metal seal surface not
holding
Up very well. Is this observed on other products from the same
manufacturer?
Do other manufacturers do this as well?
Steve
-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Monday, July 25, 2011 12:33 PM
To: 'TechNet E-Mail Forum'; 'Steven Creswick'
Subject: RE: [TN] likelihood of soic-8 package breach
I think, though I may be wrong, that plastic packages are not considered
hermetic. I thought the PRF addressed ceramic ICs with glass seals.
It's been awhile.
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Monday, July 25, 2011 12:03 PM
To: [log in to unmask]
Subject: Re: [TN] likelihood of soic-8 package breach
Chris,
Sure makes it sound like they are concerned about 'leakers' with the molded
packages, doesn't it!
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Monday, July 25, 2011 11:55 AM
To: [log in to unmask]
Subject: [TN] likelihood of soic-8 package breach
Hello netters,
If a SOIC-8 data sheet has a note "non-halide flux should be used" on their
suggested (Pb-free) reflow profile drawing, and close-by they mention that a
MIL-PRF-38534 hermetic version is available, should one read something into
this?
Thanks,
Chris
Chris Mahanna
Robisan Laboratory Inc.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|