The US EPA did a study before ROHS and did not recommend change and some
studies by European Universities conclude the Enviro impact was at best
neutral there is little point in going over all that again. We are where we
are.
Let me ask a different question:
Given that there are any number of possible solders, why wouldn't a company
use a different alloy to Sn/Pb if they found it had some benefit or
advantage? Actually many people have for years and nothing to do with
Pb-free. The alloys are chosen for what is in them rather than what is not
of course.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Sunday, July 24, 2011 1:55 PM
To: [log in to unmask]
Subject: Re: [TN] Lead Free solder has performed well...
Steve,
I am not going to put words in Vahid's or Ron's mouth, but I would expect
that in answer to your first question it would either be really, really
hard, if not impossible. And let's face it, it was a good marketing move,
whether it was initially intentional or not.
"...is lead-free solder the green "environmentally responsible" success that
was purported and mandated to all of us?"
The answer to that is of course NO. I think it is an unmitigated disaster
where we have traded one environmental issue for several we know even less
about - more energy use, more tin and silver mining, more silver potentially
killing micro-organisms, tin whiskers, drop failures, premature aging of
components because of manufacturing heat stress, more brittle board
materials and the list can be lengthened by others. Some of these are
straight out enviro in nature the others are indirectly because they lead to
more scrap.
Bev
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Saturday, July 23, 2011 10:37 PM
To: [log in to unmask]
Subject: Re: [TN] Lead Free solder has performed well...
Ron,
You know as well as I do, that the reason we were all told that we HAD to to
convert to lead-free, was because it was going to be the "environmentally
responsible" thing to do. It wasn't because we wouldn't be able manufacture
iPhones and the like because of the higher density and tighter lead pitches.
So I find the positive spin put out about lead-free solder after the "cows
have been let out of the barn" so to speak, interesting.
Don't you think that problems with solder shorts could be addressed by
optimizing board and pad layout, stencil specifications, printing processes,
and reflow parameters? Wouldn't have that been the answer rather than
switching to another solder alloy that has questionable environmental
benefits over tin/lead solder?
So, the question still remains (and many are still asking); is lead-free
solder the green "environmentally responsible" success that was purported
and mandated to all of us?
Steve
-----Original Message-----
From: Ron Lasky
Sent: Saturday, July 23, 2011 12:15 PM
To: [log in to unmask]
Subject: Re: [TN] Lead Free solder has performed well...
Folks,
Pete is correct. I never said lead-free implementation was a grand success.
These were Rob's words in his blog post
(http://www.designnews.com/author.asp?section_id=1389&doc_id=231199&f_src=de
signnews_gnews).
I have said repeatedly that adequate lead-free reliability has been
demonstrated for consumer products like mobile phones, PCs, portable
electronics with service lives less than 5 years. This level of reliability
has been demonstrated in numerous studies and more importantly with field
data. Vahid Goudarzi, of Motorola, stated that field reliability of
lead-free assembled mobile phones has been equal or better than leaded
assembly units. His data go back to 2001 (not 2006, Motorola started early
for reasons discussed below).
The reason Motorola shipped early with lead-free products is due to the fact
that lead-free solder does not spread as well. Because of this poorer
spreading, Motorola was able to decrease lead spacings without getting
shorts, thus increasing the amount of electrical function in a smaller
space. Since increased function in a smaller space is the defining
attribute of portable electronics, the importance of this lead-free
advantage cannot be overstated. Admittedly, lead-free's poorer wetting is a
challenge in other regards, especially hole fill in wave soldering, but the
Motorola Droid X2 could not be assembled with leaded solder, there would be
too many shorts. Since the packaging density of the iPhone and similar
devices is on a par with the Droid X2, I suspect this statement is true for
most mobile products.
I have also repeatedly stated that lead-free reliability for long term
service, mission critical devices has not been demonstrated. As a result,
these types of devices should not consider lead-free solder at this date.
I regularly discuss these topics in my blog
(http://blogs.indium.com/blog/an-interview-with-the-professor). The most
recent post shows a striking photo of leaded solders too good spreading for
portable electronics.
Cheers,
Ron
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|