Hi Julie,
Can you take a picture on the section between the BGA ball and it (component) substrate AFTER you had physically separated them.
Did you performed a dye and pry which will show that the contact is "opened" or near "open".
Regards
GA Tan
________________________________
From: TechNet on behalf of vladimir Igoshev
Sent: Fri 7/1/2011 9:28 PM
To: [log in to unmask]
Subject: Re: [TN] BGA ball dewet from substrate
I don't see the details I'd need but it could be caused by spalling at the UBM.
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: Steve Gregory <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Fri, 1 Jul 2011 07:58:48
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
Steve Gregory <[log in to unmask]>
Subject: Re: [TN] BGA ball dewet from substrate
Good Morning Julie,
I have your picture posted here:
http://stevezeva.homestead.com/Solder_dewet.jpg
That is pretty strange. I have never seen something like that!
Steve
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, June 30, 2011 8:47 PM
To: [log in to unmask]
Cc: [log in to unmask]
Subject: RE: [TN] BGA ball dewet from substrate
Thank you! Here it is, Steve.
--------------------------------
Julie Silk
Environmental Compliance Technical Program Manager Agilent Technologies
707-577-4296
[log in to unmask]
-----Original Message-----
From: Wenger, George M. [mailto:[log in to unmask]]
Sent: Thursday, June 30, 2011 5:34 PM
To: TechNet E-Mail Forum; SILK,JULIE (A-Sonoma,ex1)
Cc: Steve Gregory
Subject: RE: [TN] BGA ball dewet from substrate
Julie,
You can send your photograph to Steve Gregory who I've copied and he can post it on his site that is available to all the IPC TN members
Regards,
George
George M. Wenger
Senior Principal Reliability / FMA Engineer Andrew Corporation - Wireless Network Solutions 40 Technology Drive, Warren, NJ 07059
(908) 546-4531 Office (732) 309-8964 Mobile
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk
Sent: Thursday, June 30, 2011 6:29 PM
To: [log in to unmask]
Subject: Re: [TN] BGA ball dewet from substrate
The substrate pad shows an intermetallic layer, demonstrating that there had been a metallurgical bond. Also, the surface of both pad and ball are smooth -- not a fracture, but as if reflowed. I have a good picture from the FA report to share once I figure out how. I believe that if you were to analyze the very first layer on the BGA substrate pad, it would have a layer of solder.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|