Ditto,
I would appreciate a copy.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, July 01, 2011 6:34 PM
To: [log in to unmask]
Subject: Re: [TN] Solderpaste Storage and Use
Hi Mike,
You must know that I would like a copy...
Steve
-----Original Message-----
From: Mike Fenner
Sent: Friday, July 01, 2011 5:38 PM
To: [log in to unmask]
Subject: Re: [TN] Solderpaste Storage and Use
Hi all
Just to return to this thread. I have a PowerPoint presentation on storage
and best handling procedures, which documents and discusses the issues
raised here.
Note: my delay in offering it is due to it not originally being intended for
direct public use. Therefore, I asked a "respected 'Netter" for his opinion.
He has suggested minor edits to make it less commercial and thinks it should
be OK. I have made the changes and am happy to send it to anyone that would
like a copy.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Thursday, June 23, 2011 5:05 PM
To: [log in to unmask]
Subject: Re: [TN] Solderpaste Storage and Use
I just used tape...
I know what you mean about cleaning the sludge off the rollers...
That's why I got the o-rings...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Thursday, June 23, 2011 6:01 AM
To: [log in to unmask]
Subject: Re: [TN] Solderpaste Storage and Use
Paul,
Okay. You are putting the o-rings on the jars! Gotcha! I thought you were
putting them on the rollers.
I guess that I have been lucky in having containers of uniform jar/lid
diameter, but will pay extra attention to yours & Steve G's word of caution
about lids coming off. I would be seriously put out if a jar full of Ag and
glass frit slobbered out all over the rollers. I have smaller jars, having
much less mass than a jar of solder paste, too.
Wonder if it would be anal and give the lid/jar interface a quick wrap with
Parafilm?
Steve Creswick
http://www.linkedin.com/in/stevencreswick
616 834 1883
From: Paul Edwards [mailto:[log in to unmask]]
Sent: Wednesday, June 22, 2011 8:54 PM
To: 'TechNet E-Mail Forum'; 'Steven Creswick'
Subject: RE: [TN] Solderpaste Storage and Use
Actually o-rings are to keep the lids from touching the rollers and present
a uniform diameter for rolling...
I never thought about the traction thing...
I may have some car modelers donating their used tires if they read this...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Wednesday, June 22, 2011 3:36 PM
To: [log in to unmask]
Subject: Re: [TN] Solderpaste Storage and Use
Hmm! Never had that problem.
The most recent one is still rollin'
Must have been a jar-lid malfunction...
I can see how the o-rings will increase the 'traction' between the rollers
and objects being rolled.
Proper material/stock turnover is really the ideal way to go.
Steve Creswick
http://www.linkedin.com/in/stevencreswick
616 834 1883
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
_____
This email and any attachments thereto may contain private, confidential,
and privileged material for the sole use of the intended recipient. Any
review, copying, or distribution of this email (or any attachments thereto)
by others is strictly prohibited. If you are not the intended recipient,
please contact
[log in to unmask]<mailto:[log in to unmask]>
immediately and permanently delete the original and any copies of this email
and any attachments thereto.
_____
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
===========================================================================
==
This email and any attachments thereto may contain private, confidential,
and privileged material for the sole use of the intended recipient. Any
review, copying, or distribution of this email (or any attachments thereto)
by others is strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this email
and any attachments thereto.
===========================================================================
==
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives For additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|