Bubbles can be caused by these conditions as well as a host of other variables. While the experiments are going in to drive the factors to ground you should assess if you have bridging or not The intention of the term indicates non-isolation of devices - generally if you see a series of bubbles the thickness is adequate as you can discern CC between the gaps = coverage. The test for a large event must be to break and assess the coating integrity.
Jeffrey Bush
BAE Systems Incorporated
Electronic Systems Division
IS&R - Space Products and Systems
P.O. Box 868, MER24-01G43
Nashua, NH 03061-0868
Office +1 603.885.8137
Mobile +1 603.318.8056
Fax +1 603.885.5258
-----Original Message-----
From: Temkin, Gregg [mailto:[log in to unmask]]
Sent: Thursday, July 14, 2011 10:36 AM
To: [log in to unmask]; Bush, Jeffrey D. (US SSA)
Subject: RE: [TN] IPC-A-610 Conformal Coating - Coverage
How would you determine that you "...still have the minimum thickness on the conductor..." to allow you to say breaking (cured?) bubbles is OK? It's awfully difficult to measure conformal coat thickness on the sides of DIP leads or solder joints.
IMO the bubble bridging requirement is clear. If there's a bubble bridging between adjacent leads, it's a defect for Class 3. If you break the cured bubble, you're performing a repair, unless it's in your process to do it that way, but again, it's risky because you don't know if the leads or solder joints that were formerly in the bubble are truly coated.
I would fix the process to fix the problem. Bubbles can be caused by excessive application thickness or putting coated boards in a curing oven too soon after, or coating warm boards and a few other reasons that would be specific to the conformal coating system.
Gregg
-----Original Message-----
From: Bush, Jeffrey D. (US SSA) [mailto:[log in to unmask]]
Sent: Thursday, July 14, 2011 5:39 AM
To: [log in to unmask]
Subject: Re: [TN] IPC-A-610 Conformal Coating - Coverage
Bridging would indicate a reduction in the minimum surface coating requirement on either end. So it you break the bubble and you still have the minimum thickness on the conductor you are OK.
Jeffrey Bush
BAE Systems Incorporated
Electronic Systems Division
IS&R - Space Products and Systems
P.O. Box 868, MER24-01G43
Nashua, NH 03061-0868
Office +1 603.885.8137
Mobile +1 603.318.8056
Fax +1 603.885.5258
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lum Wee Mei
Sent: Thursday, July 14, 2011 3:34 AM
To: [log in to unmask]
Subject: [TN] IPC-A-610 Conformal Coating - Coverage
Dear All,
Can some kind souls help me to interpret the below statement taken out
from IPC-A-610 Section 10.5.2.2 Conformal Coating - Coverage? I am look
at Class 3 and I am loss on its interpretation, especially 'Voids or
bubbles'.
Acceptable - Class 1, 2, 3
No bridging of adjacent lands or conductive surfaces from :
* Loss of adhesion (mealing)
* Voids or bubbles
* Dewetting
* Cracks
* Ripples
* Fisheyes or orange peel
It is common to find bubbles trapped between the soldered leads of those
gull-leaded components and between closely mounted SMDs passives for
brushing method. Are these bubbles allow for Class 3?
Thanks and regards,
~wee mei~
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|