TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Rex Waygood <[log in to unmask]>
Date:
Thu, 21 Jul 2011 15:25:12 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Message-ID:
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
MIME-Version:
1.0 (Apple Message framework v1084)
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (92 lines)
Aw, Rex - you're just being cynical.

Keep in mind that the replacement alloy, when it gets into the waste stream, will not have anything like the adverse effects lead....

....so that's alright then?

Science & Reason - whooosh! Out of the window.

Graham N

On 20 Jul 2011, at 08:33, Rex Waygood wrote:

> Of course they probably get plenty of other things.
> I think one of the other major contaminants from the poor recycling of WEEE waste is dioxin. I am sure many of us saw the TV programmes showing the poor recycling of western generated WEEE waste in India, Africa and China.
> The removal of lead has done nothing for the millions of tonnes of legacy electronics still a potential for feeding the illegal recycling trade.
> Whilst we still permit the export of WEEE waste dressed up as 2nd hand goods to countries where poor recycling takes place there is little or no environmental benefit that I can perceive from the removal lead in electronics. It is my understanding that one of the custom built WEEE recycling factories in the UK is running at half capacity whilst we still ship container loads of disguised electronic scrap to the countries mentioned. Each container reportedly earning thousands of pounds for the shipper of this material.
> So possibly a better way of spending our £millions would have been to address and police the recycling chain. It seems to me that the environmental benefit would have been achieved quicker rather than the headline grabbing publicity stunt that best describes the removal of lead in electronics.
> 
> As they say, IMHO
> 
> Rex
> 
> 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
> Sent: 19 July 2011 18:55
> To: [log in to unmask]
> Subject: Re: [TN] Lead Free solder has performed well...
> 
> I think it likely the poor beggars who hand incinerate WEEE in third world, including China, to recover metals do benefit from not getting lead poisoning. The surrounding environment will benefit from reduction in heavy metal contamination also. Of course they probably get plenty of other things. 
> I don't think anyone has quantified these benefits especially as it doesn't officially happen in some of those places.
> 
> Regards
> 
> 
> Mike
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
> Sent: Tuesday, July 19, 2011 6:37 PM
> To: [log in to unmask]
> Subject: Re: [TN] Lead Free solder has performed well...
> 
> Gary,
> Excellent question to which my answer is I don't know, but I doubt it.
> Bev
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Gary Crowell
> Sent: Tuesday, July 19, 2011 12:33 PM
> To: [log in to unmask]
> Subject: Re: [TN] Lead Free solder has performed well...
> 
> For all of the debate on the performance of lead-free, the question remains:
> For all of the billions spent on process changes to eliminate lead, has there been any measurable benefit in health and safety?
> 
> Gary
> --
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2