TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Roger Tingler <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Tingler <[log in to unmask]>
Date:
Fri, 29 Jul 2011 10:12:38 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (74 lines)
Ken,

Try Taconic's RF301 and RF30 or Arlon's AD300A or CLTE-XT
But believe you my have an issue with Arlon's product out-gassing


Roger Tingler
Methods Engineer
Colonial Circuits
V:800-578-9602 x102
 540-752-5511x102
F:540-301-2050
  540-752-2109
E-mail: [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kenneth J. Wood
Sent: Friday, July 29, 2011 9:52 AM
To: [log in to unmask]
Subject: [TN] High Vacuum Substrate

Hi all,

I have a PCB that operates inside a vacuum chamber under ultra high vacuum.

The material can't outgas and needs to hold up physically under the pressure (or lack thereof).

I wanted to use RO3003 but may need something else, any suggestions?

Material lead time is an issue as well which is why I'm looking...
Thanks

Ken

_____________________________________

Kenneth J. Wood

Saturn PCB Design, Inc.

www.saturnpcb.com









______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2