Rich,
It's more complicated than you would think... There are 2 measurements, static and dynamic. Static will give you an indication how well a material will wet a surface, but you nee to know the surface energy of the substrate you are trying to wet. Best method is contact angle measurement on known surface energy substrate.
Dynamic will tell you how quickly a material will wet and flow... Especially important in processes involving rapid rearrangements, such as spraying. Best method to measure is using bubble tensiometers.
The equipment is not that expensive so if you plan on doing regularly may make sense to invest... One off, put it back on your material supplier, they should have both methods on hand.
Depends on which problem you are trying to solve. Call me if you want to discuss some more to make sure you get most meaningful data...
Best regards,
Phil.
+44 7703 795422
Sent from my iPhone
On 14 Jul 2011, at 19:27, Richard Kraszewski <[log in to unmask]> wrote:
> Can anyone provide with a name(s)?
>
> Not looking to do this on surface but rather in a bulk volume (beaker).
>
> Thanks
>
> Rich Kraszewski / PLEXUS
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|