彭主席:您好!
久没有见面,近来可好!
瓷片电容碎裂以前我碰到和处理过,与厂家有关,不同厂家同样103电容层数也不统一。当然与贴装工艺也有关系。谢谢!
陈智东
----- Original Message -----
From: "Leesha "Lixia" PENG" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, July 13, 2011 10:34 AM
Subject: [TGAsia] 转发: [TN] Capacitor Crack
> 各位TGAsia坛友,
>
> TechNet邮件论坛,于1995年建立,目前有850位注册者。以下摘自该论坛的讨论有关陶瓷电容裂纹,推荐的论文可从以下链接下载http://www.avx.com/docs/techinfo/cracks.pdf。如果有坛友知道哪里可以获得此文译稿,或翻译此文,请提交IPC中国,我们可以刊登在《电子工艺技术》杂志。谢谢!
>
> 提供此链接的David Hillman 认为,所有组装工程师都当阅读此文。
>
>
> Thanks and Best Regards
>
> Leesha PENG 彭丽霞
> GM IPC China
> IPC中国总经理
> 18616593891
>
>
> -----邮件原件-----
> 发件人: TechNet [mailto:[log in to unmask]] 代表 [log in to unmask]
> 发送时间: 2011年7月13日 7:51
> 收件人: Technet
> 主题: Re: [TN] Capacitor Crack
>
> Dave,
> Thanks for the compliment, that old paper was written in 1985 or so and is still true today. If we can get a photo up to see a better bit of advise could be supplied.
>
> Regards,
>
> John Maxwell
>
> On Tue, 12 Jul 2011 11:42:29 -0500, "David D. Hillman"
> <[log in to unmask]> wrote:
>
>
>> Hi JB - read this reference paper by John Maxwell - it should be
>> required reading for all assembly engineers:
>>
>> http://www.avx.com/docs/techinfo/cracks.pdf
>>
>>
>> Dave Hillman
>> Rockwell Collins
>> [log in to unmask]
>>
>>
>>
>> J B Ribeiro <[log in to unmask]> Sent by: TechNet
>> <[log in to unmask]>
>> 07/12/2011 11:23 AM
>> Please respond to
>> TechNet E-Mail Forum <[log in to unmask]>; Please respond to J B Ribeiro
>> <[log in to unmask]>
>>
>>
>> To
>> <[log in to unmask]>
>> cc
>>
>> Subject
>> [TN] Capacitor Crack
>>
>>
>>
>> Hi to all,
>>
>> We are problems with capacitor crack (0805).
>> The crack is 45°, close to solder pad and the initiation crack is from
>> down to top.
>>
>> What are the solutions to solver the problem?
>> Thermal Shock, Pick and Place, Depaneling?
>>
>> What is the checklist to audit my supplier?
>>
>> thank you a lot
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
>> unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
>> per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives For additional information, or
>> contact Keach Sasamori at [log in to unmask] or
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
>> unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
>> per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives For additional information, or
>> contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|