Hi Jean-Francois,
It has to be analyzed. Otherwise you will never know what went wrong.
You can contact me off line if you want to.
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: Jean-Francois Bissonnette <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Wed, 6 Jul 2011 15:37:02
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
Jean-Francois Bissonnette <[log in to unmask]>
Subject: [TN] Poor gold plating, any solution to help soldering
Hello technetters,
We received a batch of PCBs that are extremely hard to solder. The wetting
on the SMT components is fine however, the through hole is a real pain. We
tried rubbing the pads with an eraser but no results.
If the problem comes from too little gold plating, is there a solution to
help with soldering?
Thank you!
(BTW… for those who answered on the stencil issue. I’ll send questions when
I put out some other fires!!!)
Jean-François
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|