Hello technetters,
We received a batch of PCBs that are extremely hard to solder. The wetting
on the SMT components is fine however, the through hole is a real pain. We
tried rubbing the pads with an eraser but no results.
If the problem comes from too little gold plating, is there a solution to
help with soldering?
Thank you!
(BTW… for those who answered on the stencil issue. I’ll send questions when
I put out some other fires!!!)
Jean-François
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------