What is surface finishing? Black pad?
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Wenger, George M. [mailto:[log in to unmask]]
Sent: Thursday, June 30, 2011 06:13 PM
To: TechNet E-Mail Forum <[log in to unmask]>; Joyce Koo
Subject: RE: [TN] BGA ball dewet from substrate
Joyce,
It can't be head on pillow if I read Julie's comment that the separation is between the ball and the component not PCB substrate.
Julie,
Exactly what is the failure analysis signature? Is the solder ball "dewet" from the package or does the solder ball have a brittle fracture separation at the component Substate?
Regards,
George
George M. Wenger
Senior Principal Reliability / FMA Engineer
Andrew Corporation - Wireless Network Solutions
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 Office (732) 309-8964 Mobile
E-mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Thursday, June 30, 2011 6:06 PM
To: [log in to unmask]
Subject: Re: [TN] BGA ball dewet from substrate
Is it called head on pillow?
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Julie Silk [mailto:[log in to unmask]]
Sent: Thursday, June 30, 2011 06:05 PM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] BGA ball dewet from substrate
We have a failure analysis of "dewet" for a BGA ball that is separated from the component substrate. Does anyone know more about this failure mode? The part goes through reflow twice, so once while upside down. It seems unusual, even unlikely, for separation to occur between the balls and the substrate due to the weight of the part rather than between the ball and the PCB. Other parts on the same board do not have this issue. Do you have any experience with this problem or how to prevent it? Or for the future, how to predict it and thus avoid it? Would vapor phase processing influence the likelihood of this defect? Any help appreciated!
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|