TECHNET Archives

June 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Stadem, Richard D." <[log in to unmask]>
Date:
Thu, 2 Jun 2011 09:22:08 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Barbara Burcham <[log in to unmask]>
Message-ID:
Subject:
From:
Barbara Burcham <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (83 lines)
Thanks everyone for you imput. What a great group of people!

Richard,
The application will be double sided, fine pitch array components, some
through hole components and going into a shock environment.
I will need to connect with the assemblers to check on flux and paste
compounds. Does this information help?  You make an excellent point. Must
have the total picture. I do not know, yet, how long boards will sit on the
shelf before moving into assembly, either. I do know that shelf life
will also impact this decision.
I do not think that I want to use tin...that hairy growth stuff.
Barbara



On Thu, Jun 2, 2011 at 8:01 AM, Stadem, Richard D. <[log in to unmask]>wrote:

> Barbara,
> What is the application, board type, component types, etc?
> Immersion silver is my personal favorite, but that is completely
> irrelevant.
> You should choose a board finish dependent upon the application of the CCA,
> whether it has fine-pitch array components, including CSPs, whether it is
> double-sided with PTH parts or hand-soldered components, the environment the
> CCA will be used in, the flux type to be used, the alloy that is required,
> and several other factors that go into the decision. Without complete
> knowledge of all these factors, it is hard for anyone to answer that
> question. I can tell you that IAg beats ENIG in cost, but each finish has
> strengths and weaknesses. Some definitely have more or less than others.
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Barbara Burcham
> Sent: Wednesday, June 01, 2011 8:17 PM
> To: [log in to unmask]
> Subject: [TN] Best Board Finish - beyond gold
>
>  Hey Y'all,
> I am looking for a reliable bare board finish that beats the cost of gold.
> What experience is out there?
> What would you recommend?
> Thanks,
> Barbara Burcham
> pcb Trace Design
> [log in to unmask]
>
>
>  ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2