Wow, the 8 hour limit is really tight in my opinion.
I agree never to go back into cold storage once the container has been
opened, but if the seal is not broken, no moisture would have been
introduced and it is eligible to be stored if you find you don't need
it.
My paste supplier actually has documented guidelines for these
requirements.
FIFO with tubes is the best way to go, but some of us have to use
containers....
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roger Mack
Sent: Monday, June 20, 2011 12:12 PM
To: [log in to unmask]
Subject: Re: [TN] Solderpaste Storage and Use
Most pastes have a refrigeration spec. which gives it a shelf life of 6
months. If you are using 600g tubes most datasheets will require 8 hours
to acclimatise. Once out of the fridge we don't return it either, but
always sign initials, date and time on each tube. Create an out of
fridge
"on deck" storage for 3 or 4 tubes, or a daily amount for a line. We use
a
fixture that fills from the top and you pull tubes from the bottom like
a
canned drink dispenser. If you take one, add a new one to the top from
the
fridge. You will never run into trouble with your acclimitizing time, or
pull too much. Your paste likely has a shelf life for room temperature,
so
set a spec. that discards all open tubes when pulled, for say, two weeks
or a month. If you are using jars and storing working paste, sign and
date it as well and control the out of fridge time for that as well.
Roger Mack P.Eng.
Manufacturing Specialist
Parker Hannifin Canada
Electronic Controls Division
1305 Clarence Avenue
Winnipeg, MB R3T 1T4 Canada
direct 204 453 3339 x373
[log in to unmask]
www.parker.com/ecd
From:
Amol Kane <[log in to unmask]>
To:
<[log in to unmask]>
Date:
06-20-2011 13:27
Subject:
[TN] Solderpaste Storage and Use
Sent by:
TechNet <[log in to unmask]>
I am re-writing our solderpaste use and storage procedures for water
soluble and no clean fluxes (SnPb and Lead-free) to say, in essence the
following:
"To be stored per the manufacturer's recommendations (usually upto 10C),
must be at room temperature before it is dispensed on the stencil (at
least an hour thawing is required). Maximum use period to be 8 hours.
Re-refrigeration and use beyond 8 hours not permitted"
The pushback is to the prohibition of re-refrigeration (for use the next
day) after it is thawed and use beyond 8 hours requirement. These
requirements are due to concerns with moisture absorption by the
solderpaste once thawed (affecting slump) and flux activity (due to
ageing)
What criteria are all the learned folks on technet using for solderpaste
management? Is there any literature available that looks at solderpaste
use limits on time and temperature?
A logical solution would be to do a DOE to look at these parameters, but
I
am being asked to come up with something ASAP:). love how these things
work!
Thanks in advance
Amol
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
"PLEASE NOTE: The preceding information may be confidential or
privileged. It only should be used or disseminated for the purpose
of conducting business with Parker. If you are not an intended
recipient, please notify the sender by replying to this message and
then delete the information from your system. Thank you for your
cooperation."
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|