I have also seen where we stockpiled the particular x-out by panel
location so that they could all be run at the same time.
Another option was to punch out the fiducials on the x-outs and have the
pick and place recognize which to populate.
We typically always had four up ABAB configuration panels and only one
x-out was ever allowed.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McGlaughlin, Jeffrey
A
Sent: Monday, June 06, 2011 11:19 AM
To: [log in to unmask]
Subject: Re: [TN] X-Out Policy
Our typical stance is no X-out on low board count arrays (generally
fewer than 4 boards per array). For higher part count arrays no more
than 2 x-outs per array and no more than 10% of ordered quantity in
x-outs.
Jeffrey A McGlaughlin, CID
Engineering Designer
Systems Development Engineering Services
Room 4-2-50
Phone (614)424-7582
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Monday, June 06, 2011 11:22 AM
To: [log in to unmask]
Subject: [TN] X-Out Policy
These is a debate currently raging on internally on whether or not to
allow X-outs on panelized assemblies. I am of the opinion to not allow
any X-outs as this entails manual intervention on the line to not
populate that particular board (we have not programmed any bad board
sense into our programs), and to a lesser extent, leads to solderpaste
wastage. Furthermore, to me, accepting X-outs means accepting a more
variable (if not a out of control) process at the board house. However,
I want to to hear to any opinions otherwise if any
What is the industry doing as a whole regarding X-outs?
Thanks,
Amol
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|