DESIGNERCOUNCIL Archives

June 2011

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
DesignerCouncil <[log in to unmask]>
X-To:
Designers Council Forum <[log in to unmask]>, Andy Kowalewski <[log in to unmask]>
Date:
Thu, 9 Jun 2011 06:22:44 -0700
Reply-To:
"(Designers Council Forum)" <[log in to unmask]>, Tom Garman <[log in to unmask]>
Subject:
From:
Tom Garman <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (177 lines)
A lot of these consumer products are getting good at meeting the intent of the mil/hi reliabilty requirements without a lot of the added expense.
Most of the engineers I work with have never seen a mil spec, but they know that when a guy drops his GPS, it bounces off the boat and goes in the water. When the guy fishes it out he expects it to work again.

Best Regards;
Tom G.

--- On Wed, 6/8/11, Andy Kowalewski <[log in to unmask]> wrote:

> From: Andy Kowalewski <[log in to unmask]>
> Subject: Re: [DC] Underfill for chip scale packages
> To: [log in to unmask]
> Date: Wednesday, June 8, 2011, 8:57 PM
> Makes sense. So it (corner bonding)
> would be applied to packages that are a
> bit bulky (=heavier than normal) and maybe don't have so
> many pins to absorb
> drop shock?
> 
> Thanks Steve.
> 
> Cheers........
> 
> Andy Kowalewski
> AdvantagePCB Pty Ltd
> +61 (2) 9499 4853
> 
> -----Original Message-----
> From: DesignerCouncil [mailto:[log in to unmask]]
> On Behalf Of Steve
> Gregory
> Sent: Thursday, 9 June 2011 09:06
> To: [log in to unmask]
> Subject: Re: [DC] Underfill for chip scale packages
> 
> Hi Andy,
> 
> Corner bonding, not underfill. It helps with surviving drop
> shock without 
> having to go through all the trouble of underfilling.
> Corner bonding is lots
> 
> easier to do...
> 
> Steve
> 
> -----Original Message----- 
> From: Andy Kowalewski
> Sent: Wednesday, June 08, 2011 6:53 PM
> To: [log in to unmask]
> Subject: [DC] Underfill for chip scale packages
> 
> Just saw a web knock-down of the Barnes and Noble eBook
> reader. The larger
> Chip Scale Packages appear to have underfill applied to
> each corner, which
> has me intrigued. See
> 
> 
> 
> http://www.techrepublic.com/photos/cracking-open-the-2011-barnes-noble-nook-
> e-book-reader-wi-fi/6243892?seq=35
> <http://www.techrepublic.com/photos/cracking-open-the-2011-barnes-noble-nook
> -e-book-reader-wi-fi/6243892?seq=35&tag=content;thumbnail-view-selector>
> &tag=content;thumbnail-view-selector
> 
> 
> 
> Does anyone know the criteria for this? Underfill is
> applied in flipchip
> assembly to prevent the silicon cracking because of the
> thermal mismatch in
> CTE between glass (3ppm/degree C) and pcb (FR4 at about
> 16ppm/degreeC). I
> guess the CSP might have a similar issue - no doubt the
> silicon chip inside
> the package also gets stressed as the package stresses,
> which implies that
> there isn't a lead frame to give compliance, or a FR4
> laminate interposer
> like in bga packages that doesn't need stress relief.
> 
> 
> 
> Cheers........
> 
> 
> 
> Andy Kowalewski
> 
> AdvantagePCB Pty Ltd
> 
> +61 (2) 9499 4853
> 
> 
> 
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email
> Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
> 
> ----------------------------------------------------------------------------
> -----
> DesignerCouncil Mail List provided as a free service by IPC
> using LISTSERV 
> 16.0.
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil
> send: SET 
> DesignerCouncil NOMAIL/(MAIL)
> For additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> ----------------------------------------------------------------------------
> ----- 
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email
> Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> 
> ______________________________________________________________________
> 
> ----------------------------------------------------------------------------
> -----
> DesignerCouncil Mail List provided as a free service by IPC
> using LISTSERV
> 16.0.
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil
> send: SET
> DesignerCouncil NOMAIL/(MAIL)
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> ----------------------------------------------------------------------------
> -----
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email
> Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> 
> ______________________________________________________________________
> 
> ---------------------------------------------------------------------------------
> DesignerCouncil Mail List provided as a free service by IPC
> using LISTSERV 16.0.
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil
> send: SET DesignerCouncil NOMAIL/(MAIL)
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> ---------------------------------------------------------------------------------
> 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2