Craig,
We have been using the products from Shercon with good results. The green
polyester tape is what we have been using and it seems to work well with
both Humiseal 1B31 and Humiseal 1H20AR1. It has a max temp of 400F, but
that is well above most coating cure steps I know of.
http://www.shercon.com/storefront/PC21Greenployestertape.aspx
They also sell this green tape in rolls of squares and round dots of
varying sizes. In a couple years of use, we have had no problems with
residues or left behind adhesive.
Doug Pauls
Rockwell Collins
Craig Sullivan <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/16/2011 08:34 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Craig Sullivan <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
[TN] Conformal Coat tape
Well, I suppose this is a repeat from a few years ago when Humiseal
stopped selling their conformal coat tape and left everyone searching for
alternatives.
Recap: Humiseal HT-500 tape was manufactured exclusively for Humiseal by
St. Gobain. The St. Gobain part number is M797. St. Gobain had numerous
quality issues and as such Humiseal ceased the line. St. Gobain continues
to manufacture the tape. We had continued to use the St. Gobain part with
minor quality problems here and there. We decided to live with the issues
because the tape works so well with our Acrylic coating.
Fast forward to today: St. Gobain decided to put the tape on a liner to
correct various issues they and other customers had. Problem is we now see
excessive residue left on the boards as well as the rolls falling apart if
we're not careful with handling. They've also scaled back production and
as such the lead times have quadrupled.
So, my question is can anyone share what they use with their acrylic
coatings? We use a boat load of this stuff so I need to find a seamless
replacement.
Thank you,
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480
F: 607.266.0482
[log in to unmask]<mailto:[log in to unmask]>
P Please consider the environment before printing this e-mail.
________________________________
Confidentiality Notice:
This e-mail contains privileged and confidential information which is the
property of MPL Incorporated, intended only for the use of the intended
recipient(s). Unauthorized use or disclosure of this information is
prohibited. If you are not an intended recipient, please immediately
notify MPL Incorporated and destroy any copies of this email. Receipt of
this e-mail shall not be deemed a waiver by MPL Incorporated of any
privilege or the confidential nature of the information.
Export Control:
This message is intended only for the addressee and may contain
information that is company confidential or privileged. Any technical data
in this message may be exported only in accordance with the U.S.
International Traffic in Arms Regulations (22 CFR Parts 120-130) or the
Export Administration Regulations (15 CFR Parts 730-774). Unauthorized use
is strictly prohibited and may be unlawful. If you are not the intended
recipient, or the person responsible for delivering to the intended
recipient, you should not read, copy, disclose or otherwise use this
message. If you have received this email in error, please delete it, and
advise the sender immediately.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|