Technetters, I'm looking at part of IPC-4101C. Slash sheet /29.
For resin system, it lists 'Primary: epoxy', 'Secondary1: cyanate ester', Secondary2:N/A'.
Looking through the body of 4101, I see 7.2 has a table for 'material composition keywords' with 'epoxy/cyanate ester/woven glass' associated with /29.
Is 4101 saying that /29 material has a resin system which contains BOTH epoxy AND cyanate ester in a single sheet of laminate or prepreg?
As always, I appreciate any guidance from you ladies and gentlemen.
Louis Hart
Compunetics
Monroeville, PA
USA
[log in to unmask]<mailto:[log in to unmask]>
412-858-1272
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|