Blair,
Provided you, or the operators, are comfortable with transferring the partial contents of the squeezie bottles to 30cc syringes [use a piston in the syringe so there is less chance of sucking latex back into the valve if they have the vac pull-back on], they should be happy to use an EFD [or similar] dispenser.
Now you have to pay for disposable syringes, pistons and needles, however.
Steve Creswick
http://www.linkedin.com/in/stevencreswick
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------