Hi Steve-
You are talking about a design problem, not a handling problem. These devices are actually much more robust than alternative GaAsFET devices commonly used at somewhat lower frequencies. I had one about 6 years ago that would blow up with only 9V of static!
The design issue is that the parts must be protected against static once they are soldered in. This is easy to do inherently because the ramp rate of the static discharge is much slower than the frequency of interest. So a simple inductor is often used to protect the terminals without causing problems with the RF. If some aspect of the design renders this impossible, then place a deliberate short across the vulnerable terminals and cut it free when the external connections are made (and if they don't protect against static discharge, then the thing won't work very long anyway).
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gene Felder
Sent: Tuesday, April 12, 2011 1:26 PM
To: [log in to unmask]
Subject: Re: [TN] Class 0 ESDS board assembly transport...
Grounding works great. However, cart drag chains are problematic. It might
be more effective to purchase conductive casters.
A cart cover having shielding properties would not be necessary if all
conductors are effectively grounded, and all insulators are removed from the
ESD protected area.
Gene Felder
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard D. Krug
Sent: 2011 - 04 - 12 10:10 AM
To: [log in to unmask]
Subject: Re: [TN] Class 0 ESDS board assembly transport...
I don't know how much additional protection the cover provides. Perhaps an
ESD blanket to cover CCA's on dissipative trays could provide cost effective
protection if you don't have large numbers of these large CCA's.
Dick Krug, CSMTPE
SMT Process Engineer
Sparton Corporation
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, April 12, 2011 12:27 PM
To: 'TechNet E-Mail Forum'; Richard D. Krug
Subject: RE: [TN] Class 0 ESDS board assembly transport...
Hi Dick,
Yeah, I think I saw those for Metro tray carts:
http://www.metro-wire.com/index.cfm?mf=browse.showPart&partClassID=5363&PNam
e=SmartTray%20ESD%20Cart%20Covers
The carts that I was considering earlier were 18" X 26" Bliss tray carts,
and they only have 5-sides too. But I found out that the 18" X 26" tray
isn't big enough for the largest boards we build here.
http://catalog.blissindustries.com/cgi-bin/Panorama.cgi?CATALOG~.catpart~976
0-300-11
Bliss says they will do a custom cover, but I haven't got a quote back from
them yet (everybody is at APEX).
The covered cart option is pretty expensive, and I'm wondering how much
extra protection (if any) that really buys you.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard D. Krug
Sent: Tuesday, April 12, 2011 12:03 PM
To: [log in to unmask]
Subject: Re: [TN] Class 0 ESDS board assembly transport...
In my past we had used some ESD cloth covers over racks with CCA's. CCA's
were not Class 0. Covers were over 5 sides, but I think the bottom was
open.
Dick Krug, CSMTPE
SMT Process Engineer
Sparton Corporation
30167 Power Line Road
Brooksville, FL 34602-8299
p (352) 540-4012 (Internal Ext. 2012)
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, April 12, 2011 11:56 AM
To: [log in to unmask]
Subject: Re: [TN] Class 0 ESDS board assembly transport...
I know a lot are off to APEX, but do any of you have any opinion of tray
carts moving product on the production floor? Specifically in a low ESD
sensitive environment?
Do covered carts offer any more protection than a open cart if it is well
grounded and the product is on static dissipative trays?
Just trying to understand if I need to spend the extra money on a covered
cart or not.
Thanks,
Steve
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|