It's been my experience that the SIR and ROSE results I get for test
coupons washed in 2 Mohm cm water are considerable better than the result
obtained after washing with city water, This would also depend on the
particular city water, some are better than others.
Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069
Re: [TN] Aqueous Wash, DI water and IPC Specifications.
Robert Kondner
to:
TechNet
04/21/2011
06:46 PM
Sent by:
TechNet <[log in to unmask]>
Please respond to rkondner
Hi,
From what I have read and heard it is ionic content on the board after the
rinse/dry cycle that matters. That means you need an idea of final rinse
dissolved solids content (assume they are all ionic) and how much water
remains on the board after the rinse cycle. If you have an air knife or
blowing system that removes most of the rinse water then it does not matter
what you rinse with.
From the amount of water I could measure on a PCB after rinse and blow off
even the worse tap water is fine for rinse as the final board is very
clean.
Ok, now all the DI Rinse Only folks can start throwing rocks.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Forrester, Michael (H
USA)
Sent: Thursday, April 21, 2011 6:17 PM
To: [log in to unmask]
Subject: Re: [TN] Aqueous Wash, DI water and IPC Specifications.
Dave,
For water washable fluxes, where cleaning is required, is DI
water
REQUIRED per IPC? IPC-AC-62A section 13.3 Final Rinse: implies DI water,
section
10.6 I'm not
sure what it implies. It states DI is preferred and then goes on to say it
(refering to DI water) doesn't have to be ultra pure (18.2 MegOhm-cm) and
that
1 to 5 MegOhm-cm is satisfactory. 1-5 MegOhm-cm DI water a min.
REQUIREMENT? I
have one side saying IPC spec REQUIRES DI water and the other side saying
IPC spec only recommends/prefers DI water. It is basically a compliance
issue.
If DI water
is not used in the aqueous wash is that a violation of IPC specifications?
Best Regards,
Michael Forrester
Sr. Product Engineer
CSMTPE
Siemens Healthcare Diagnostics
101 Silvermine Rd.
Brookfield, CT 06804
PH: (203) 740-6452
-----Original Message-----
From: David Bealer [mailto:[log in to unmask]]
Sent: Thursday, April 21, 2011 5:56 PM
To: TechNet E-Mail Forum; Forrester, Michael (H USA)
Subject: RE: [TN] Aqueous Wash, DI water and IPC Specifications.
As I read IPC-610E; cleaning is not a requirement, as Flux residues from
no-clean processes are acceptable for classes 1,2,& 3.
We require our assemblies to meet IPC class 2, however we separately
require
those same assemblies to meet specific cleanliness requirements because of
the end use environment. To meet those cleanliness requirements we use a
water washable flux, and an inline recycling water wash system where the
final rinse water is a minimum of 2Mohm.
BR,
David Bealer | SMT Department Manager
Phone: (217) 442-0611 ext. 6022 | Fax: (217) 477-7134
Watchfire Signs by Time-O-Matic Inc.
[log in to unmask]
www.watchfiresigns.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Forrester, Michael
(H USA)
Sent: Thursday, April 21, 2011 4:06 PM
To: [log in to unmask]
Subject: Re: [TN] Aqueous Wash, DI water and IPC Specifications.
What I'm trying to find out is do IPC specifications REQUIRE
DI water?
Best Regards,
Michael Forrester
Sr. Product Engineer
CSMTPE
Siemens Healthcare Diagnostics
101 Silvermine Rd.
Brookfield, CT 06804
PH: (203) 740-6452
-----Original Message-----
From: Woolley, Mark D. (Mark) [mailto:[log in to unmask]]
Sent: Thursday, April 21, 2011 4:57 PM
To: TechNet E-Mail Forum; Forrester, Michael (H USA)
Subject: RE: [TN] Aqueous Wash, DI water and IPC Specifications.
Unless DI water is continuously cleanses and filtered, DI water will
decrease in resistivity due to disolved CO2. I believe that clean water
without dissolved ions should be used for celaning, but it does not have
to meet the DI water standard of 20Mohm resistivity as would be required
for a wafer process.
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster, CO 80234 USA |
Voice (Lab): (303) 538-2166 | email: [log in to unmask] |
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Forrester, Michael
(H USA)
Sent: Thursday, April 21, 2011 1:36 PM
To: [log in to unmask]
Subject: [TN] Aqueous Wash, DI water and IPC Specifications.
I have a question about aqueous wash. There is a difference of opinion
on what IPC REQUIRES as far as wash water. The main issue is does IPC
specifications REQUIRE or PREFER/RECOMMEND DI water for aqueous wash?
IPC-AC-62A I don't think is clear. The spec in section 10.6 states:
"Rinse Water Parameter: Good quality deionized water is the
preferred rinse medium. However, this is not meant to suggest that
ultapure, 18.2 megohm-cm water is necessary. Water in the 1 to 5
megohm-cm region will be satisfactory for most operations"
The same spec in section 13.3 states:
"Final Rinse: This cleaning step is where the board is subject to
purified DI water rinse."
The PCBA print basically calls out build to IPC-610 class 2 and does not
call out any specific cleaning specifications. So, with all that said,
Is it an IPC REQUIREMENT to use DI water for aqueous wash? Thank you.
Best Regards,
Michael Forrester
Sr. Product Engineer
CSMTPE
Siemens Healthcare Diagnostics
101 Silvermine Rd.
Brookfield, CT 06804
PH: (203) 740-6452
------------------------------------------------------------------------
-------
This message and any included attachments are from Siemens Healthcare
Diagnostics
and are intended only for the addressee(s).
The information contained herein may include trade secrets or privileged
or
otherwise confidential information. Unauthorized review, forwarding,
printing,
copying, distributing, or using such information is strictly prohibited
and may
be unlawful. If you received this message in error, or have reason to
believe
you are not authorized to receive it, please promptly delete this
message and
notify the sender by e-mail with a copy to
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
-------
This message and any included attachments are from Siemens Healthcare
Diagnostics
and are intended only for the addressee(s).
The information contained herein may include trade secrets or privileged
or
otherwise confidential information. Unauthorized review, forwarding,
printing,
copying, distributing, or using such information is strictly prohibited
and may
be unlawful. If you received this message in error, or have reason to
believe
you are not authorized to receive it, please promptly delete this
message and
notify the sender by e-mail with a copy to
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
----------------------------------------------------------------------------
---
This message and any included attachments are from Siemens Healthcare
Diagnostics
and are intended only for the addressee(s).
The information contained herein may include trade secrets or privileged or
otherwise confidential information. Unauthorized review, forwarding,
printing,
copying, distributing, or using such information is strictly prohibited and
may
be unlawful. If you received this message in error, or have reason to
believe
you are not authorized to receive it, please promptly delete this message
and
notify the sender by e-mail with a copy to
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|