My question is: do the rest of the BGA balls look like pumpkins and
these corner balls are stretched and leaning towards the middle?
A 900 pin bga is large enough I can envision some corner movement
potential due to package movement.
I don't know of any specific reject paragraph which would apply to this
condition but when approving up a new reflow process, my preference is
to have the BGA cross sectioned so that I could compare the height of
the balls along the entire side (and across the middle as well).
Sometimes xray images can be very deceiving and actual cross sections
resolve any doubt.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, April 27, 2011 11:33 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Ball Tilt
Hi Mark,
I have your pictures up on my web page:
http://stevezeva.homestead.com/corner_1_45_degrees.jpg
http://stevezeva.homestead.com/corner_2_135_degrees.jpg
and in looking at your images, I don't know that I see a real problem
there.
The ball shape may not be perfectly symmetrical, but I see the same sort
of
shape in the other two balls in each image.
Maybe others can look at these images and say if there's anything to be
too
concerned about...
Steve
-----Original Message-----
From: Woolley, Mark D. (Mark) [mailto:[log in to unmask]]
Sent: Wednesday, April 27, 2011 12:51 PM
To: Steve Gregory
Subject: RE: [TN] BGA Ball Tilt
Steve,
The X-ray images are taken 60degrees to the beam direction. The
magnification is geometric not mathematical. These are same side
corners
(not opposite corners).
Thanks,
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster,
CO 80234 USA | Voice (Lab): (303) 538-2166 | email: [log in to unmask]
|
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, April 27, 2011 10:03 AM
To: 'TechNet E-Mail Forum'; Woolley, Mark D. (Mark)
Subject: RE: [TN] BGA Ball Tilt
Do you have any pictures Mark?
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Woolley, Mark D.
(Mark)
Sent: Wednesday, April 27, 2011 11:56 AM
To: [log in to unmask]
Subject: [TN] BGA Ball Tilt
I am experiencing a BGA condition I have never encountered before. A
large
>900 pin BGA has corner pins that are not perpendiculat to the PWB
surface.
They are slightly angled toward the center of the BGA. This is seen on
all
four corners. Obviously, this condition is not preferred. Is there a
specification that states the condition of the ball?
Thanks,
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster,
CO 80234 USA |
Voice (Lab): (303) 538-2166 | email: [log in to unmask] |
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|