Kimberly:
I believe we are the only company supplying an Immersion Palladium plating system.
This system is a true immersion Palladium, and plates only on bare Copper. It is not ENEPIG. It has had limited use, and great results, and has been shown to maintain solderability for years. By comparison to ENEPIG is is extremely inexpensive, and is ridiculously easy to maintain.
If you send me a a street address, I would be pleased to send you a brochure on the system.
Regards,
Rudy Sedlak
--- On Wed, 4/20/11, Kimberly Stanley <[log in to unmask]> wrote:
From: Kimberly Stanley <[log in to unmask]>
Subject: [TN] Immersion/Electroless Palladium as final finish?
To: [log in to unmask]
Date: Wednesday, April 20, 2011, 1:13 PM
Hi all.
Has anyone heard of using immersion or electroless palladium as a replacement for an ENIG or electroplated nickel/gold final finish? I've been asked to research it but I'm having trouble finding any information. I've only heard of palladium being used as a component of an ENEPIG finish.
Thanks,
Kim
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|